WTB-Flatness Gauge
Currently refurbishing a Lapping Machine and I am looking to purchase a flatness gauge if anyone has one laying around??? Regards All Norm
-
4th Jan 2021, 01:07 PM #2Golden Member
- Join Date
- Sep 2008
- Location
- Riddells Creek, Vic.
- Posts
- 838
Do you want an Optical Flat or some sort of Mechanical/Electronic gauge?
-
4th Jan 2021, 01:33 PM #3Member
- Join Date
- Jan 2017
- Location
- Bunbury
- Posts
- 63
I have some optical flats, what I am looking for is is a mechanical gauge such as the Lap Master have. With Regards Norm
-
4th Feb 2021, 12:12 AM #4Member
- Join Date
- Jan 2017
- Location
- Bunbury
- Posts
- 63
I have managed to purchase a Lapmatster flatness gauge. Thank you to all who may have been looking on my behalf. Regards to All. Norm
Similar Threads
-
Jig to measure flatness ?
By steamingbill in forum METALWORK PROJECTSReplies: 5Last Post: 9th Aug 2018, 11:43 PM -
Cast Iron Pot Flatness
By electrosteam in forum GENERAL DISCUSSION / OFF TOPICReplies: 11Last Post: 25th Jul 2017, 08:28 PM -
Recommended reading please : flatness - accuracy - straightness
By steamingbill in forum METALWORK GENERALReplies: 9Last Post: 20th Feb 2013, 06:40 PM -
How do I test it for flatness?
By jmk89 in forum METALWORK GENERALReplies: 27Last Post: 20th May 2010, 05:33 PM -
Measuring flatness of plate
By Dengue in forum METALWORK GENERALReplies: 9Last Post: 22nd May 2009, 09:16 PM