Results 1 to 9 of 9
  1. #1
    Join Date
    May 2011
    Location
    Murray Bridge S Aust.
    Age
    71
    Posts
    5,959

    Default Hardened Drill Guides

    Wanting to buy 3 drill guides, size number 11 for the pop rivets, if anyone has a few laying around. Preferably with a collar to stop them falling through.
    Can't seem to find them on Fleabuy, either that or I'm looking for the wrong thing.
    Thanks in Advance,
    Kryn
    To grow old is mandatory, growing up is optional.

  2. #2
    Join Date
    Sep 2008
    Location
    Riddells Creek, Vic.
    Posts
    838

    Default

    I didn't think that anyone in Australia would still be making drill bushes, but apparently, at least one company does: https://www.fjbushings.com.au/

  3. #3
    Join Date
    Aug 2006
    Location
    Melbourne
    Posts
    1,106

    Default

    Would the inner section of a bearing be suitable as a drill guide?

  4. #4
    Join Date
    May 2011
    Location
    Murray Bridge S Aust.
    Age
    71
    Posts
    5,959

    Default

    I suppose it would do, just a matter of finding some that size. 4.85 mm or .191" could be a tricky thing to find. Will speak to the bearing blokes tomorrow.
    Thanks,
    Kryn
    To grow old is mandatory, growing up is optional.

  5. #5
    Join Date
    Mar 2011
    Location
    Southern Flinders Ranges
    Posts
    1,555

    Default

    I have some 7/8” 4140 I acquired recently, I could cut a few small pieces off and put a #11 hole through it for you if that would work?

  6. #6
    Join Date
    Aug 2006
    Location
    Melbourne
    Posts
    1,106

    Default

    Quote Originally Posted by KBs PensNmore View Post
    I suppose it would do, just a matter of finding some that size. 4.85 mm or .191" could be a tricky thing to find.
    Will speak to the bearing blokes tomorrow.
    Thanks,
    Kryn
    I was just curious if the bearing material would be suitable for the purpose, not sure they would have something suitable in the size you are after.

    I have some 16mm diameter holes to drill soon and finding a bearing with that ID wouldn't be too difficult.

  7. #7
    Join Date
    Oct 2011
    Location
    Norwood-ish, Adelaide
    Age
    59
    Posts
    6,561

    Default

    Quote Originally Posted by Com_VC View Post
    I was just curious if the bearing material would be suitable for the purpose, not sure they would have something suitable in the size you are after.
    It really depends on how much use the jig will get as to whether bearing steel would work. Certainly better than MS though. The big problem with using a bearing inner is that they are quite squat, so hole alignment becomes harder. You also need to secure them. Most drill guides are either long enough (2 to 3x diameter) to push into a frame or have a flange for attachment.

    Michael

  8. #8
    Join Date
    May 2011
    Location
    Murray Bridge S Aust.
    Age
    71
    Posts
    5,959

    Default

    Quote Originally Posted by racingtadpole View Post
    I have some 7/8” 4140 I acquired recently, I could cut a few small pieces off and put a #11 hole through it for you if that would work?
    Thanks Adam, I'm getting Michael to make up some for me.
    Thanks again.
    Kryn
    To grow old is mandatory, growing up is optional.

  9. #9
    Join Date
    May 2011
    Location
    Murray Bridge S Aust.
    Age
    71
    Posts
    5,959

    Default

    The jig gets used quite often, 3 holes per plate. It's used for making the clearance light plates on trailers. Recently did 22 plates for the one trailer, some take only 6 but on average about 10 per trailer, times that by 6 trailers a month, = 180 holes per month.
    Trying to talk boss into getting a punch and shear machine is like pulling teeth!!!!!!
    Kryn
    To grow old is mandatory, growing up is optional.

Similar Threads

  1. Guides for installing and setting up a mill?
    By takai in forum METALWORK GENERAL
    Replies: 3
    Last Post: 25th Mar 2020, 08:21 PM
  2. valve guides
    By morrisman in forum METALWORK GENERAL
    Replies: 20
    Last Post: 13th May 2017, 06:13 PM
  3. turning hardened steel
    By tanii51 in forum THE HERCUS AREA
    Replies: 3
    Last Post: 24th Jul 2009, 12:04 AM
  4. Milling hardened steel
    By glock40sw in forum METALWORK GENERAL
    Replies: 14
    Last Post: 26th Jul 2007, 04:46 PM
  5. Hydraulics - learning guides
    By Clinton1 in forum METALWORK GENERAL