Hi,
I need to cut a M32 x 2.0mm thread into brass, one time only, long story, thread on a coffee machine boiler is a little out of spec.
I can't seem to find a tap in Aus for this.
Obviously because I only need it one time I want to keep the cost down.
I tried to order one for $50 on aliexpress but I have cancelled that now as I believe the coronavirus has massively impacted the ETA.
Thanks for looking.
Cheers
Richard
-
15th Feb 2020, 05:19 PM #2Most Valued Member
- Join Date
- Oct 2010
- Location
- melbourne, laverton
- Posts
- 1,910
haha. hi mate . how are you.
maybe mate may be. ill look tommorow.
aaron
-
15th Feb 2020, 05:31 PM #3Most Valued Member
- Join Date
- Oct 2010
- Location
- melbourne, laverton
- Posts
- 1,910
emmm ive got one in my hand at the moment. Its a nice one. Its an intermediate and sharp.
ill send a pm.
aaron
-
15th Feb 2020, 08:22 PM #4Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,959
If you've stuff like that laying around, maybe you want to look at hiring them out.
Never know there could be a market for that type of thing??To grow old is mandatory, growing up is optional.
-
15th Feb 2020, 10:29 PM #5Most Valued Member
- Join Date
- Oct 2010
- Location
- melbourne, laverton
- Posts
- 1,910
thats funny kryn. sort of makes sence. when i read like metric fine i thought ive got that for sure probaby lh and rh.
-
15th Feb 2020, 10:51 PM #6Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,959
Odd sized stuff that's not being used and people requiring the use of one but not wanting to outlay big bucks for one.
Could be the start of a small business for you.
KrynTo grow old is mandatory, growing up is optional.