Thanks: 0
Needs Pictures: 0
Results 1 to 13 of 13
Thread: Help needed
-
1st Oct 2019, 07:46 PM #1
Help needed
Gday members
First I have my first lathe it's a qualos Australian built lathe. But I have found a worn gear in the carriage apron. Would anybody know of some spare parts for sale or would any members have a hobb that would be interested in giving me a quote on making a new one.
Thanks
Stewart
-
1st Oct 2019, 08:04 PM #2Most Valued Member
- Join Date
- Jul 2016
- Location
- Melbourne
- Age
- 35
- Posts
- 1,522
Would you be able to pop up the gear specs like number of teeth, diametral pitch and gear style (I'm assuming it's a spur gear?) As well as material I'm sure one of us can help.
-
1st Oct 2019, 08:34 PM #3Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,561
A hob is not the only way to make a gear. As Ralph said, put up some sizes and a pic or two and someone should be able to help.
Michael
-
1st Oct 2019, 09:20 PM #4
Thanks for the reply. It's a (or was) a worm wheel gear made or cast iron I can't measure the pitch because it is so bad but a rough measurement is on od of 2 inches. How do you post pictures? I have them all on my phone but can't work out how.
Last edited by sims; 1st Oct 2019 at 09:21 PM. Reason: Spelling
-
1st Oct 2019, 10:23 PM #5Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,561
When you go to reply to thread there is either a paperclip that lets you attach things or the picture looking button in the second row
Annotation 2019-10-01 205334.jpg
So (roughly) 2" OD; how many teeth and how wide are the teeth. Is there a hole through the centre or is it on a shaft?
Michael
-
2nd Oct 2019, 09:32 AM #6
Thanks Michael I should of said I'm using my phone, maybe I need the app I will try downloading it tomorrow.
The gear has a bore through it and is sized at .750 there where 22 teeth the total gear depth is .970 it has a counterbore bore at one end and a internal taper at the end which acts as a cone clutch. This engages drive to the cross slide. I hope this makes a little more sense hopefully I can post pictures soon.
Again thanks for your help.
Stewart
-
2nd Oct 2019, 10:41 AM #7
Hi Stewart, if you scroll to the bottom of the page, you’ll see a link to take you to the “Full Site”, once you’ve done that, you’ll see the options that Michael is talking about
Cheers
DJ
-
2nd Oct 2019, 11:02 AM #8
Wow thanks!!!!!! now lets see if I can work this out!
-
2nd Oct 2019, 07:29 PM #9Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,561
The pictures help, so thanks for that.
That certainly is worn. Not sure how it would have gotten that bad but these things happen
I'd be willing to have a look at it for you, although you would be up for postage and maybe something for material.
Michael
-
3rd Oct 2019, 09:14 AM #10
Thanks Michael I have sent you a message.
Stewart
-
3rd Oct 2019, 05:24 PM #11Gear expert in training
- Join Date
- Aug 2008
- Location
- Melbourne
- Age
- 34
- Posts
- 1,080
I'll put my hand up as a second option if Michael can't. I was actually doing a one-off worm/wheel set at work yesterday and today
-
3rd Oct 2019, 05:29 PM #12
Thanks for the offer will keep you in mind!
-
10th Oct 2019, 09:15 AM #13Most Valued Member
- Join Date
- Jul 2006
- Location
- Athelstone, SA 5076
- Posts
- 4,258
another happy member thanks to the generosity of our some of much appreciated talented members
Similar Threads
-
Help needed, PLEASE.
By KBs PensNmore in forum METALWORK GENERALReplies: 4Last Post: 7th May 2018, 05:51 PM -
Possible Help Needed
By matthew_g in forum METALWORK GENERALReplies: 2Last Post: 11th Apr 2018, 12:54 AM -
Help needed with DRO set up
By TED C in forum METALWORK GENERALReplies: 6Last Post: 16th Jun 2015, 03:51 PM -
help needed
By kdalton1 in forum WELDINGReplies: 10Last Post: 27th Apr 2015, 08:47 PM -
help needed please.
By danielhobby in forum METALWORK GENERALReplies: 6Last Post: 9th Oct 2013, 11:18 PM