Making right hand lathe tools
My far east import lathe tool has reached the end of it's useful life.
The material was all too soft and the pocket for the insert is badly deformed.
So I make a new holder using tough tool steel.
I also make another lathe tool by brazing the carbide tip on a steel shank.
There is a video presentation of the process here
In this video I am using:
- Weiler Matador SV (1972) Lathe
- Schaublin SV-51 (1955) Milling machine
Similar Threads
-
second hand tools /machinery
By daggagh in forum METALWORK GENERALReplies: 7Last Post: 24th Oct 2019, 11:13 PM -
Japanese second hand tools market
By caskwarrior in forum METALWORK GENERALReplies: 3Last Post: 24th Oct 2018, 09:22 AM -
Buying hand tools from the US
By TheOtherLeft in forum METALWORK GENERALReplies: 8Last Post: 7th May 2011, 12:32 PM -
Making some of your own hand tools
By Grahame Collins in forum WELDINGReplies: 20Last Post: 5th Feb 2008, 06:32 PM