2nd May 2021, 05:23 PM #1
Ham Radio Tower Top Pulley Replacements
Hi All.
I have just made some replacement pulleys for a mate that live 10m up the top of his antenna tower, the original pulleys were made of plastic;
IMG_2186-1.jpgIMG_2187-1.jpgIMG_2188-1.jpgIMG_2185.jpg
So it's no wonder the plastic unit failed in the harsh Australian sun, full view of the UV's up there.
I had some 80mm dia aluminum stock so I cut some off and into the lathe;
IMG_2168.jpgIMG_2169.jpgIMG_2170.jpg
These should last a bit longer than the last ones, the biggest issue I had was parting them off, my parting tool left me with about 30mm to hacksaw through, I ground a piece of tool steel to make the grooves, it all worked out in the end, they are installed and functioning and he is rather chuffed with it all
So then I had a mess to clean up as usual, I do like to keep my machines clean;
IMG_2171.jpgIMG_2172.jpgIMG_2173.jpg
A pleasant afternoon spent playing in the workshop enjoying some machine therapy
Cheers all
Peter
Similar Threads
-
welding podcast radio show
By meadow street in forum WELDINGReplies: 0Last Post: 23rd Aug 2016, 12:14 PM -
Pulley ideas
By morrisman in forum METALWORK GENERALReplies: 24Last Post: 7th Apr 2016, 12:29 AM -
Workshop LIghting .. LED Replacements for Fluoroescent Tubes
By RayG in forum METALWORK GENERALReplies: 48Last Post: 4th Jun 2015, 06:52 PM -
SOLD: Alloy Pulley
By eskimo in forum METALWORK - Machinery, Equipment, MARKETReplies: 4Last Post: 6th Jan 2012, 08:31 AM -
Pulley Modification
By Anorak Bob in forum METALWORK GENERALReplies: 14Last Post: 29th Jan 2011, 07:29 PM