I had having problems replacing damaged 1/4 inch zerk oilers on my lathe.
I brought some from a E-bay seller.
The first one was too tight and I mangled it, the second I pressed in but it was too long and restricted topslide travel.
I could have brought Alemlube 1/4 inch fittings from E-bay for $21.30 but I need 4, and they may not have fitted.
So I brought 20 6mm brass oilers from Alibaba for $5.00 and modified them to suit.
Once off the lathe I silver soldered them together, the white stuff covering the ball is old fashioned liquid paper (Kryptonite for solder).
MarkI've become a tool of my tools.
-
3rd Feb 2021, 05:36 PM #2Most Valued Member
- Join Date
- Mar 2011
- Location
- Southern Flinders Ranges
- Posts
- 1,555
Thanks, I learnt something. Had no idea silver solder could be dammed with Liquid paper.
-
3rd Feb 2021, 10:29 PM #3Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 57
- Posts
- 2,672
Good work - I’d have taken the chicken (loctite) option
Any issues with the springs after the silver soldering?
Steve
-
4th Feb 2021, 12:37 AM #4
Soldering
Steve I used a Weller 51D soldering station, cranked up to 45 watts and had no problems with the spring and ball mechanism.
I've done 3 so far