    Default Rolling stand

    Over the last few months (almost a year) I've been doing a job for Bob (China). He managed to get hold of a pair of jewellery rolls; could I make up a frame for them?
    Today I managed to do the last of the tricky bits, so here it is.
    DSCN7414 (Small).JPG DSCN7413 (Small).JPG
    The gears on the top are to synchronise the two screws that push the rolls down.
    The rolls themselves are synchronised with the two gears in the photo below. M5 - probably the largest tooth size I've ever cut. They go on the two stub shafts in the photo and then the cover at the back goes on (this thing will be motor driven, so no chances with mashing a finger)
    DSCN7416 (Small).JPG
    A little bit of tweaking to go but substantially done. Most of the steel is reclaimed from some injection moulding dies that a neighbour gave me a year or so back, so there are a few holes here and there that make no sense but there is a reason for that.

    Michael
    (Trying out new 'shed' camera with new improved lighting - no flash used)

  2. #2
    Join Date
    Aug 2011
    Location
    Melbourne
    Posts
    4,597

    Default

    Hi Michael,

    That looks like a work of art. Very solid. Nice work.

    Excuse my ignorance but what does it do?

    Simon

    Sent from my SM-G970F using Tapatalk
    Girl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.

  3. #3
    Join Date
    Oct 2011
    Location
    Norwood-ish, Adelaide
    Age
    56
    Posts
    5,937

    Default

    I just make them...
    From what I was told, precious metal is cast or supplied as wire. These rolls are to reduce it down to a desired size. The grooves in the ends of the rolls allow the wire to be shaped to a D or other shape if it is there.

    My estimate for what is there is just north of 50kg, so yes, solid.

    Michael

  4. #4
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    1,366

    Default

    That is coming along nicely Michael, another twenty kilo's for the motor and gearbox, for those who asked have a look here it gives the basic understanding of what it is used for
    https://www.youtube.com/watch?v=BsfJYi-G1D8

  5. #5
    Join Date
    Jan 2004
    Location
    Mackay North Qld
    Posts
    5,827

    Default

    Nice one, Michael!

    Grahame

  6. #6
    Join Date
    Oct 2011
    Location
    Norwood-ish, Adelaide
    Age
    56
    Posts
    5,937

    Default

    Added the depth indicator today. Using a feeler gauge, it even seems to be 'accurate'.
    DSCN7482 (Small).JPG
    (Al disc attaches to the handle shaft with a split cotter. Numbering with the engraving pantograph; divisions with my division scriber thing.)

    Michael

  7. #7
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    1,366

    Default

    looking good I have almost got a space for it.

  8. #8
    Join Date
    Jan 2021
    Location
    uk
    Age
    34
    Posts
    1

    Default

    Quote Originally Posted by Michael G View Post
    Over the last few months (almost a year) I've been doing a job for Bob (China). He managed to get hold of a pair of jewellery rolls; could I make up a frame for them?
    Today I managed to do the last of the tricky bits, so here it is.
    DSCN7414 (Small).JPG DSCN7413 (Small).JPG
    The gears on the top are to synchronise the two screws that push the rolls down.
    The rolls themselves are synchronised with the two gears in the photo below. M5 - probably the largest tooth size I've ever cut. They go on the two stub shafts in the photo and then the cover at the back goes on (this thing will be motor driven, so no chances with mashing a finger)
    DSCN7416 (Small).JPG
    A little bit of tweaking to go but substantially done. Most of the steel is reclaimed from some injection moulding dies that a neighbour gave me a year or so back, so there are a few holes here and there that make no sense but there is a reason for that.

    Michael
    (Trying out new 'shed' camera with new improved lighting - no flash used)
    good job

  9. #9
    Join Date
    Jul 2011
    Location
    Adelaide
    Posts
    736

    Default

    Industrial art. It looks perfect.

  10. #10
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    1,366

    Default

    Machine is painted and up and running see Jewellery forum

  11. #11
    Join Date
    Dec 2007
    Location
    Adelaide
    Posts
    372

    Default

    Nice work you should give yourself a pat on the back.

  12. #12
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    1,366

    Default

    Any pats on the back go to "Michael G." he built it, I just, did the less than perfect paint job.

Similar Threads

  1. Plate rolling
    By KBs PensNmore in forum METALWORK GENERAL
    Replies: 13
    Last Post: 14th Dec 2018, 01:52 AM
  2. Rolling rings from 8mm rod
    By Scally in forum METALWORK GENERAL
    Replies: 13
    Last Post: 1st Jan 2017, 08:13 PM
  3. Rolling copper
    By denncarm in forum METALWORK GENERAL
    Replies: 5
    Last Post: 27th Oct 2013, 05:15 PM
  4. Rolling Tailstock Arbor
    By barkersegg in forum METALWORK GENERAL
    Replies: 5
    Last Post: 9th Dec 2011, 08:22 AM
  5. Rolling brass plate
    By SHIPPERS in forum METALWORK GENERAL
    Replies: 0
    Last Post: 23rd Oct 2009, 06:04 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •