Needs Pictures: 0
Results 1 to 4 of 4
-
28th Nov 2020, 09:47 PM #1Diamond Member
- Join Date
- Aug 2019
- Location
- Revesby - Sydney Australia
- Age
- 57
- Posts
- 1,196
How NOT to adapt a lathe carriage-stop
I bought a cheap stop from China:
https://www.aliexpress.com/item/32982044383.html
IMG_1054.jpg
Probably for a Sieg lathe. Was hoping it would clamp on my Hercus V, but it's too small:
IMG_1055.jpg
So I thought I would try to mill it out. First, mount and clock: IMG_1056.jpg
Then, try to mill out the clearance slot.
Will a single clamp hold it? No, no it didn't: IMG_1057.jpg
OK. I'll try a dodgy old machine vice. I don't have any parallels, so I'l try to fudge it:
IMG_1058.jpg
(then it got too hot, so I stopped for the day. Will continue the story on Monday)
-
29th Nov 2020, 12:43 AM #2Senior Member
- Join Date
- Aug 2012
- Location
- Greenmount, W.A.
- Age
- 70
- Posts
- 275
I made a Hercus stop from a short piece of 25x25 square bar, and a M6x1 threaded rod for adjusting the stop. Didn't take long to make.
Parallels. Old bearings, and bearing rollers, and HSS make cheap parallels. They can be made too. There was an article in Model Engineering Workshop about that. I would need to search for the issue.
-
3rd Dec 2020, 08:26 PM #3Diamond Member
- Join Date
- Aug 2019
- Location
- Revesby - Sydney Australia
- Age
- 57
- Posts
- 1,196
Milled out the slot a bit more:
IMG_1064.jpg
Then upgraded to a borrowed, tilting, vice:
IMG_1065.jpg
for opening up the V:
IMG_1066.jpg IMG_1067.jpg
which seemed to do OK. Not a perfect surface finish, but for a blunt old 10mm cutter, good enough:
IMG_1068.jpg
Now, onto the other block...
IMG_1072.jpg IMG_1073.jpg
OK. Assemble and test:
IMG_1074.jpg IMG_1075.jpg
A quick crank of the carriage showed that it didn't grip very well.
1) Tried tightening the M6 lever clamp as much as I dared. A gentle push from the saddle will feel you are at the stop, but I can't imagine when actually cutting something – pushing a cutter into hot metal – that it would restrict very much.
2) Tightened it a lot more. It almost does the job, but looking closely shows that the back of the top half is lifting away from the V.
3) Hacky solution, using what I had on hand:
IMG_1076.jpg
Summary: A clamp designed for a 15mm? V isn't strong enough for the Hercus's 20-ish-mm wide V
-
4th Dec 2020, 12:48 PM #4
There a some good examples of lathe stops made by forums members on this site including mine.
https://metalworkforums.com/f303/t20...ndicator-mount
I have since slotted the stop bar and added matching pin to the body to stop the dial indicator rotating during adjustment.
MarkI've become a tool of my tools.
Similar Threads
-
Carriage stop bolt
By ptrott in forum METALWORK GENERALReplies: 6Last Post: 22nd Jun 2020, 03:36 PM -
Carriage Stop Clamp Plates
By Anorak Bob in forum THE HERCUS AREAReplies: 8Last Post: 29th Apr 2020, 10:51 PM -
Micrometer carriage 'stop'
By Michael G in forum METALWORK PROJECTSReplies: 0Last Post: 10th Sep 2016, 04:59 PM -
How does this work ? Micrometer Carriage Stop.
By auscab in forum THE HERCUS AREAReplies: 4Last Post: 31st May 2015, 08:26 PM -
Four Position Carriage Stop
By localele in forum THE HERCUS AREAReplies: 5Last Post: 6th May 2015, 09:10 PM