    Hi all,

    I've had this DH for some time now. It was thrown in with a "pile of stuff" when I bought my mill. It was in very bad condition and at the time I thought it was scrap metal. Anyway I did my usual, took it apart and cleaned it. With some TLC it got it turning a while back. It still has some issues and one of them was the sliding retainer thingy that holds the indexing pin.

    Originally it was one piece cast in with the turn handle but someone obviously broke it off. It had been "repaired" with what looks like a combination of silver solder and welding but it since broke off again as it was in the box of "stuff".

    Today I made a new piece. I decided to keep the original handle (because I couldn't bring myself to throw it) and fit and screw another piece to it.

    I was concerned it would look terrible and not be strong enough but I surprised myself. I'm happy with the result.





    Sent from my SM-G970F using Tapatalk
    Girl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.

  2. #2
    Join Date
    Feb 2014
    Location
    Werribee, Melbourne
    Posts
    178

    Default

    Nice save!

  3. #3
    Join Date
    Nov 2019
    Location
    Brisbane
    Age
    69
    Posts
    452

    Default dividing head

    That is a well engineered repair. And a nice finish.
    Regards
    BC

  4. #4
    Join Date
    Aug 2011
    Location
    Melbourne
    Posts
    4,779

    Default

    Thanks guys for your kind words and encouragement!

    I'm off to use it now to make a couple of hand knobs for my pan brake project.

    Having a 3 jaw chuck, its much easier than clamping stuff on a RT.

    Simon

    Sent from my SM-G970F using Tapatalk
    Girl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.

  5. #5
    Join Date
    Aug 2011
    Location
    Melbourne
    Posts
    4,779

    Default

    Couple of adjustment knobs for the pan brake. They are not gears or anything of tight tollerance but it seems to work ok.

    Simon

    Sent from my SM-G970F using Tapatalk
    Girl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.

Similar Threads

  1. How to use a semi Universal Dividing rotary head
    By KBs PensNmore in forum METALWORK GENERAL
    Replies: 0
    Last Post: 28th Jun 2019, 03:38 PM
  2. FS Mecha Dividing Head Semi Universal.
    By achjimmy in forum METALWORK - Machinery, Equipment, MARKET
    Replies: 2
    Last Post: 1st Jul 2017, 02:31 PM
  3. More pre-dumpster diving
    By BobL in forum METALWORK GENERAL
    Replies: 7
    Last Post: 29th Jun 2016, 11:38 AM
  4. Replies: 15
    Last Post: 14th Jul 2014, 08:13 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •