    Inspired by the make it extreme youtube series I was sick breaking vices so I decided to build my own.

    It is nothing special but it is very strong and should last a lifetime...or two

    I built it out of scrap from the local recyclers. So besides the acme threaded rod and a couple of thrust bearings it owes me next to nothing, which is well within my price range

    Pile of scrap



    Some of the actual build









    And of course a stand that suits the vice..





    And the finished article.....and a pic to give a size reference







    I made both soft jaws and hardened steel jaws for it. I havent bolted it down yet as I am unsure where to commit to that but as it is with a stand full of concrete and solid lump of steel for the vice it weighs so much it doesnt really move a lot just sitting there!

    And I have also removed the paint from the top anvil section and polished it...it looks so pretty it was a shame to use it, but like everything in my garage it now looks quite second hand.

  2. #2
    BobL is online now Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,189

    Default

    The shed is Waaaaaaaay too tidy.

    Vice looks great

  3. #3
    Join Date
    Oct 2019
    Location
    Tasmania
    Age
    53
    Posts
    150

    Default

    Quote Originally Posted by BobL View Post
    The shed is Waaaaaaaay too tidy.

    Vice looks great
    Thanks Bob, its not always clean, sometimes you cant move in there when I am doing a project. I do feel like I spend most of my life tidying up though

  4. #4
    Join Date
    Nov 2007
    Location
    Near Rockhampton
    Posts
    270

    Default

    With that list of Bathurst winners I'm guessing there's a Ford in the shed as well.

  5. #5
    Join Date
    Nov 2004
    Location
    Bungama SA
    Age
    52
    Posts
    960

    Default

    Nice build looks good, where did you get the acme thread from?
    ....................................................................

  6. #6
    Join Date
    Oct 2019
    Location
    Tasmania
    Age
    53
    Posts
    150

    Default

    Thanks gents

    I bleed blue and over the years have owned many a nice Ford but none in the shed at the moment.

    I got the acme threaded rod at our local nuts and bolts supplier and just machined they end to suit the socket I made.

  7. #7
    Join Date
    Nov 2019
    Location
    Brisbane
    Age
    69
    Posts
    452

    Default Big vice.

    That is a really good job.
    It needs a made in Aus sticker or a green and gold stripe job.
    Regards
    BC

  8. #8
    BobL is online now Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,189

    Default

    Have you done any testing?

    eg https://youtu.be/VcbTopj5u7A

  9. #9
    Join Date
    Oct 2019
    Location
    Tasmania
    Age
    53
    Posts
    150

    Default

    Aussie made sticker is a great idea

    Good video Bob. I can say with out even testing it that the force it applies by hand is massive. You wouldnt break it in million years bashing a piece of steel held by it but I have to admit putting a 6 foot bar onto the already long handle and leaning on it like that would strip the thread I think.

    EDIT: Actually it wouldnt strip the thread, the shear pins holding the outer bush onto the 1" acme threaded rod would break first

  10. #10
    Join Date
    Nov 2004
    Location
    Bungama SA
    Age
    52
    Posts
    960

    Default

    Unfortunately there's no nut n bolt specialist around these parts and if you ask the local supply shops for acme thread you will get a dumb founded look and possibly a roadrunner meep meep
    So far looking online seems to lead nowhere except to exuberantly priced CNC parts. I'll have to wait until I go to Adelaide next time(never hopefully...)

    If you want to see a HD vice the guy in the video above is currently building one thats over a 1000lb's
    ....................................................................

Similar Threads

  1. Dawn drill press vice - LARGE
    By racingtadpole in forum METALWORK - Machinery, Equipment, MARKET
    Replies: 3
    Last Post: 7th Dec 2018, 01:29 PM
  2. carter no 4 vice , pipe vice,triton saw holder
    By robyn2839 in forum METALWORK - Machinery, Equipment, MARKET
    Replies: 1
    Last Post: 27th Nov 2018, 04:27 PM
  3. Large Record vice Sydney.
    By clear out in forum METALWORK - Machinery, Equipment, MARKET
    Replies: 0
    Last Post: 1st Nov 2018, 05:50 AM
  4. Large Tandem Axle Trailer Build
    By gazza2009au in forum TRAILERS & OTHER FABRICATED STUFF
    Replies: 1
    Last Post: 18th Feb 2018, 09:29 AM
  5. help me build a basic flat build bed trailer for my kayaks
    By gros21 in forum TRAILERS & OTHER FABRICATED STUFF
    Replies: 7
    Last Post: 13th Oct 2011, 08:47 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •