    Thanks Shed.
    You’re reading it correctly.
    TBH I struggled a bit with with the setup, and was definitely grinding away from the cutting edge rather than into it.
    A lot of that was my tooth rest arrangement being less than ideal, and I think the 10mm cutter is really too small for indexing that way.
    I spent a bit of time last night making a new sleeve with a better fit in the workhead, and a larger retaining collar with indexing slots like BC showed earlier.
    I just need to cut the slots now to finish it.
    Should make the indexing easier and will allow me to use the other side of the wheel so I’ll be grinding into the edge.

    Steve

  2. #107
    Join Date
    Nov 2017
    Location
    Geelong, Australia
    Age
    57
    Posts
    2,673

    Default

    Finished off the indexing collar, then found I didn’t have enough clearance to get the index finger set up. Made up a rough holder so I could mount it higher - the same index finger I used previously slides up inside the bore.




    Was going to have a crack at this roughing endmill I buggered last year as it’s a decent size to learn on and I can’t make it any worse that it is now - but after cutting the end off with the angle grinder I realized that it’s obviously not going to fit in the ER20 holder




    So had another play with drill faceting.
    Angles aren’t right but I was happy with how the indexing worked and the finish.



    Steve

Page 8 of 8 FirstFirst ... 345678

Similar Threads

  1. A gear cutter grinding jig for tool and cutter grinder.
    By steamloco1954 in forum METALWORK GENERAL
    Replies: 1
    Last Post: 30th Mar 2020, 07:30 PM
  2. Hercus tool and cutter grinder & cylindrical grinder.
    By stix012 in forum EBAY, GUMTREE, and other off forum sales sites
    Replies: 1
    Last Post: 23rd Aug 2018, 05:31 PM
  3. Another Tool And Cutter Grinder
    By Anorak Bob in forum METALWORK GENERAL
    Replies: 26
    Last Post: 13th Nov 2013, 12:15 PM
  4. Tool and Cutter grinder
    By 4-6-4 in forum METALWORK GENERAL
    Replies: 2
    Last Post: 12th Oct 2011, 11:40 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •