Needs Pictures: 0
Results 31 to 45 of 107
Thread: Power tool and cutter grinder
-
13th Jul 2020, 01:02 AM #31Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 57
- Posts
- 2,672
Thanks BC. I've searched and found a couple of them that give me some ideas to start with.
I should also get onto ordering a couple of wheels to get me started, considering post is so slow these days.
The wheel hub fits 32mm/1.25" wheels.
I've got a few plain white and pink wheels in the 6-12mm width that I picked up a couple of years back, so should be OK there, but no real idea on cup and dish wheels.
For a start I'm planning to just concentrate on doing some HSS end mills, but will also need a diamond wheel to use for carbide ones.
White wheels in the 60-80grit range seem to be the general recommendation, and around the 180-220grit in diamond
Any recommendations on some general purpose wheels to start out with?
Steve
-
13th Jul 2020, 08:42 AM #32Senior Member
- Join Date
- Nov 2019
- Location
- Brisbane
- Age
- 69
- Posts
- 452
T & C wheels
Hello again.
11V9 flared cup wheels are good for the end of end mills and annular cutters. An angle grinder 125 X 1.6mm cut off wheel for gashing, good quality of course. Also a 100 X 50mm straight cup wheel for using the flat face. EG when grinding countersinks, taps and 4 facet drills. 38A60 KV or similar. I have tried RA or ruby wheels which are tougher and give a better finish but cut slow on good quality HSS.
A DS1 dressing stick is handy for the bench grinder wheels or tool room wheels if they just need deglazing or are loaded. Don't buy cheap brand wheels as they are rubbish. I stick to Norton or Abrasiflex. I have only recently started to grind carbide and found a 180 grit wheel a bit coarse.
Regards
BC
-
13th Jul 2020, 09:56 AM #33Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 57
- Posts
- 2,672
Awesome - thanks BC.
There are both 100 and 125mm sizes in the flared cup wheels. Any preference?
Steve
-
13th Jul 2020, 05:24 PM #34Senior Member
- Join Date
- Nov 2019
- Location
- Brisbane
- Age
- 69
- Posts
- 452
T & C wheels
Hello again.
100/75mm runs at the rite speed and the smaller wheel gets in where the big wheel won't fit. Also when grinding cutters like annular, the position of the wheel relative to cutter centre can change the distance to the following tooth. This is a bit dodgy on cutters with small spacing between flutes. Especially on annular cutters adjusting cutter tooth centre height with the index finger alters clearance to the next tooth. However it changes clearance angle and facet centre line. All a big compromise. Took me hours to get it down pat. Each cup wheel gets me about 2000 cutters so the cost is low. Dressing wears the wheel more.
Regards
BC
-
13th Jul 2020, 05:33 PM #35Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 57
- Posts
- 2,672
Cheers BC - I've just ordered both wheels online from Blackwoods.
Probably not the cheapest place to buy them, but convenient for now.
Steve
-
14th Jul 2020, 12:42 PM #36Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 57
- Posts
- 2,672
Just got a reply from Bellowflex about the column bellows.
The can do a stitched type bellows for $275 + GST
Looks like I'm going to have to keep my eye out for some poly-tarp and get the old sewing machine out myself.....
Steve
-
16th Jul 2020, 12:37 AM #37Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 57
- Posts
- 2,672
Power tool and cutter grinder
Managed to remove the motor from the bottom of the column and get it out of the base casting.
Weighs about 30kg I reckon - and I've decided its not going back in.
I'm thinking I'll combine Steamloco and BaronJ's suggestions and drive it with a DC treadmill motor mounted on the top of the spindle housing. I've got a 180v 1.5HP one here, and most of the parts to control it. Just need to pick up a bigger bridge rectifier as I don't have anything here that will handle the 7.5A
I thought about using a small 3ph motor and VFD, and even plonked the smallest spare motor (1.5kw) I've got on top to see what it would look like. Decided it would be complete overkill....
Opened up the electric panel, and felt like I'd stepped back a century.
Measured up the wheel hub as I'll need to make some more, and turns out its 3" taper per foot , with 1" diameter on the large end.
Looking online that seems to be a common size for a lot of surface and tool grinders.
Steve
-
16th Jul 2020, 05:42 AM #38
Hi Steve,
Don't forget to allow for the inrush current for the bridge rectifier. 25 amp 600 volt ones are as cheap as chips !
PS: I agree about the big blue motor in your picture, it looks enormous compared to the spindle.Best Regards:
Baron J.
-
16th Jul 2020, 06:00 AM #39Senior Member
- Join Date
- Feb 2009
- Location
- jilliby nsw
- Age
- 71
- Posts
- 111
I thought about using a small 3ph motor and VFD, and even plonked the smallest spare motor (1.5kw) I've got on top to see what it would look like. Decided it would be complete overkill....
Steve my wheel motor is only a 1/2 hp single phase and it is adequate to carry out any grinding operation I've done to date. Re motor placement, I have a plate that bolts to the wheelhead with a ribbed belt drive. I'll get a pic tomorrow
-
16th Jul 2020, 08:13 AM #40Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 57
- Posts
- 2,672
Thanks John, I've ordered a couple of the 25A ones (AU stock) which should be here early next week, and also a handful of the cheap 50A square metal case flavour with the spade lug terminals from China in case I need them later.
I was sure I had a couple here, but the largest one I could find was 8A. Likely I'll trip over one today now that I've ordered more.....
Steve
-
16th Jul 2020, 06:12 PM #41
Hi Steve,
Yes that seems always to be the case ! You are sure you have one somewhere, but can't find it until you order another one. That safe place must be bloody enormous
Just a suggestion. You’ve probably seen me mention "Shower pump motors" ! I've had half a dozen or more now, all obtained free from the local scrap yard. All 240 volt 50 Hz AC. In every case the motor has been perfectly fine. The problem has always been that the pump at one end or the other or both has sized up, usually the hot end.
These motors all seem to be in the 300 to 600 watt range, mostly induction types but a few are variable speed universal brush motors. Easily identified by having a speed control knob on them. Though I very recently got an induction motor one that has a VFD built into it, which surprised me a little.
They all seem to have 8 to 10 mm diameter shafts, so a useful size range. All the induction motor ones run at 2800/3000 rpm, whilst the universal types run around 3,5K to 4K rpm.
The good ones have bronze pumps and impellers. Which I return to the scrap yard. This is really a bit of give and take, because the bronze is worth more to the scrap man than the rest of the motors, but they are not worth his time stripping them down.Best Regards:
Baron J.
-
16th Jul 2020, 09:41 PM #42Golden Member
- Join Date
- Sep 2008
- Location
- Riddells Creek, Vic.
- Posts
- 838
Steve, you may be disappointed with the performance of the DC motor on a machine like this, I think the best option would be to convert the original motor to Delta and use a VFD. I set up my old surface grinder, which has a motor like yours, and it has been working perfectly for years.
-
17th Jul 2020, 06:38 PM #43Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 57
- Posts
- 2,672
Thanks Techo1.
I'm actually keen to give the DC motor a try. HP wise it should be overkill, and I've seen lots of videos online of guys using them as motors for linishers etc which I'd think would be a tougher gig than this grinder.
Also, with this motor being a 2-speed one, I'm not sure how its constructed - ie whether its just 2 completely separate windings or one of the Dahlander pole-changing style ones that I've just had my first encounter with on a mate's cold saw.
If its the latter then it probably can't be run on 240v anyway.
Should be minimal work to mount the treadmill motor on the top of the spindle head and drive it off the other end of the spindle and try it. I'll leave the existing drive belt in place in the column and make sure its clear of the spindle - that way if I change my mind down the track its easy to revert. I've got 415v 3ph-3ph VFDs here and a phase converter so plenty of options...
Steve
-
17th Jul 2020, 06:50 PM #44Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 57
- Posts
- 2,672
BaronJ - those shower pumps sound like a useful source of motors, but they must be a UK thing as I've never seen any down under.
Our showers generally just run straight from mains water pressure.
Steve
-
17th Jul 2020, 11:17 PM #45
Hi Steve,
They are ! The local scrap guy seems to get loads of them, mainly from jobbing plumbers. I was in there this morning and he currently has an 8 ton skip full of them. I can basically go and help myself to what ever I want, as long as he gets the bronze scrap back.
Generally the showers do run direct from mains water pressure, but there are people that like to have showers that sting like a swarm of wasps ! Of course there are also low water pressure areas where the pressure is quite low, such as living at the top of a hill.
Some of these pumps will produce 8ft head and 5 bar pressures.Best Regards:
Baron J.
Similar Threads
-
A gear cutter grinding jig for tool and cutter grinder.
By steamloco1954 in forum METALWORK GENERALReplies: 1Last Post: 30th Mar 2020, 07:30 PM -
Hercus tool and cutter grinder & cylindrical grinder.
By stix012 in forum EBAY, GUMTREE, and other off forum sales sitesReplies: 1Last Post: 23rd Aug 2018, 05:31 PM -
Another Tool And Cutter Grinder
By Anorak Bob in forum METALWORK GENERALReplies: 26Last Post: 13th Nov 2013, 12:15 PM -
Tool and Cutter grinder