help with spring valve seat manufacture, + steel sourcing S.W. Sydney
hi , i,m rebuilding my fiat tractor engine at this time. i am in the reassemble phase. i,m going to send the head off to get decked and vacuum tested (for valve sealing) . i pulled all the valves out and lapped them in good. then i took the head to pressure clean , and during this step , i,ve lost a valve spring seat. for those unaware , the valve spring sits on a hard seat, as opposed to the spring sitting on cast iron (and wearing it out). well, stupid, studip me has gone and lost one seat. i,ve looked and looked, but i can,t find it. very frustrating to say the least. fiat suppliers don,t stock this any more, its a 1976 model.
the silver lining is that i get to use my hercus lathe and make something up.
i enjoy learning new things (machining hard steel).
i,m inexperienced in this type of steel selection, and i think i will need a 4130 or 4140 steel or other?, however i would like recommendations and opinions please. the steel needs to be tough and machinable. i don,t think mild steel is tough enough, i can do better!
does anybody know where i can get this special steel stock? in S.W. Sydney or wollongong? ive used southern steel at milperra many times , not sure if they stock harder steel thou. i only need 150mm to 300mm rod/shaft will do. the seat dimensions are; 36.42mm dia, about 6mm height, and steps down to 3mm , and about 14.25mm hole.
thanks mick
-
12th Jun 2020, 08:03 PM #2Most Valued Member
- Join Date
- Jun 2007
- Location
- sydney ( st marys )
- Age
- 64
- Posts
- 4,890
Are you going to harden it when finished?
-
12th Jun 2020, 08:15 PM #3Member
- Join Date
- May 2020
- Location
- s.w. sydney
- Posts
- 53
-
12th Jun 2020, 09:23 PM #4Most Valued Member
- Join Date
- Jun 2007
- Location
- sydney ( st marys )
- Age
- 64
- Posts
- 4,890
Can't answer if it is better to or not, probably using 4140 or en36 should be fine.
A supplier in the S/W you may need to search for unless you try the steel store.
-
12th Jun 2020, 10:15 PM #5
Hi Mick, Guys,
As far as I'm aware those spring cups are not hardened ! You could check with a file on the outer edge of one.
As far as loosing one, try waving a magnet around in the general area.
I lost a M6 grub screw into the lawn, no way could I see it in the grass, a magnet found it about three feet away from where I thought it should have been.Best Regards:
Baron J.
-
12th Jun 2020, 11:11 PM #6Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 57
- Posts
- 2,671
Is it just a thin washer approx 1mm or less like used on a lot of aluminium heads, or is it thicker with possibly a profile ie not just flat?
A photo of one of its orphaned siblings would be good
Steve
-
12th Jun 2020, 11:27 PM #7Member
- Join Date
- May 2020
- Location
- s.w. sydney
- Posts
- 53
-
12th Jun 2020, 11:42 PM #8Member
- Join Date
- May 2020
- Location
- s.w. sydney
- Posts
- 53
the spring sits on a 3mm section ,similar but much thicker that a car valve spring seat. then it steps up from 3mm , to 6mm inner height. the inner height keeps the spring centralized on the spring seat . it is not flat. the spring is centralized by the washer/seat , that rises INTO the spring, to 6mm . i dont know how to post pictures.
-
13th Jun 2020, 12:00 AM #9Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 57
- Posts
- 2,671
Like this sort of shape?
https://www.enginemaster.com.au/isky...45-thick-1.540
Steve
-
13th Jun 2020, 12:15 AM #10Member
- Join Date
- May 2020
- Location
- s.w. sydney
- Posts
- 53
-
13th Jun 2020, 10:36 PM #11Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,959
Have you tried contacting either of these?
https://www.neils.com.au/fiat-tractor
https://wrights-tractor-sales.tradef....au/contact-us
KrynTo grow old is mandatory, growing up is optional.
Similar Threads
-
Sourcing Bright Flat Steel Bar
By ericg in forum METALWORK GENERALReplies: 7Last Post: 26th Sep 2014, 08:11 AM -
Supplier of high speed steel and tool steel bar and spring steel in melbourne?
By fudo133 in forum METALWORK GENERALReplies: 3Last Post: 25th Jun 2014, 12:44 PM -
looking for some spring steel
By benupton in forum METALWORK GENERALReplies: 2Last Post: 5th Feb 2011, 09:05 PM -
Spring Steel
By Big Shed in forum METALWORK GENERALReplies: 4Last Post: 8th Jul 2009, 09:01 PM -
Spring Steel
By MICKYG in forum METALWORK GENERALReplies: 9Last Post: 27th Sep 2005, 10:41 PM