Results 1 to 7 of 7
Thread: Kafer indicator
-
1st Jun 2020, 07:02 PM #1Most Valued Member
- Join Date
- Apr 2012
- Location
- Healesville
- Posts
- 2,129
Kafer indicator
I received this indicator from UK ebay the other day, it was advertised as "in excellent condition"..........
It was stuck good and proper, a clean with acetone and bit by bit it came good.
The next problem arose when I broke the placka thingo, I thought it was just being stubborn and the circlip wouldn't let it go
The placka bit is held on by 3 spring clips under the inner face and there was no way I could get that needle off and I didn't want to damage those bits as well.
Oh well....I am more into function than form so I thought I would work around it, it ended up being 1mm bigger in diameter.
This is what I did and it works like a beauty
-
1st Jun 2020, 08:00 PM #2Senior Member
- Join Date
- Feb 2014
- Location
- Werribee, Melbourne
- Posts
- 177
Nice work!
-
2nd Jun 2020, 06:11 AM #3
Hi John,
It looks beautiful ! A unique gauge I must say.Best Regards:
Baron J.
-
3rd Jun 2020, 06:24 AM #4
Excellent Lathe work! Is that one of those mini lathe machines? How does the blade hold up when you use it on metals like so?
-
3rd Jun 2020, 09:47 AM #5Most Valued Member
- Join Date
- Apr 2012
- Location
- Healesville
- Posts
- 2,129
Hi TIG, the material is phospher bronze and it is pretty easy to machine. The chuck is a 80mm mini ĺathe
chuck mounted on a backing plate with an arbour and this mounted in a 300mm 4 jaw chuck.
The lathe is much the same as this https://www.machineryhouse.com.au/l600d
The lathe and tooling thought that they were cutting air on that job.Last edited by shedhappens; 3rd Jun 2020 at 09:55 AM. Reason: text size
-
6th Jun 2020, 07:23 AM #6
-
7th Jun 2020, 03:03 PM #7Most Valued Member
- Join Date
- Apr 2012
- Location
- Healesville
- Posts
- 2,129
I think that is the best place for it, much more peaceful there than in the house..
For me (and many in this forum) yes..... but the sad truth is that most ppl these days can't even use a screwdriver so only
you could answer that question for yourself.
Similar Threads
-
Indicator holder.
By BaronJ in forum METALWORK GENERALReplies: 15Last Post: 13th Feb 2016, 08:06 AM -
Indicator Sag.
By RayG in forum METALWORK GENERALReplies: 21Last Post: 30th Sep 2015, 10:21 PM -
Indicator Point !
By BaronJ in forum METALWORK GENERALReplies: 2Last Post: 17th Dec 2014, 07:14 AM -
dial indicator
By fittermachinist in forum METALWORK GENERALReplies: 30Last Post: 12th Aug 2012, 12:20 AM -
Not a DRO - An indicator instead.
By Anorak Bob in forum METALWORK GENERALReplies: 29Last Post: 16th Nov 2011, 10:07 PM