Loco build shaper work
SAM_0614.jpgSAM_0613.jpgSAM_0612.jpgA little bleat for Saturday
My horn keeps call for 1/2X 3/8" flat bar. All I had was 25 X 10mm so over to the CMZ shaper.
Four pieces were clamped in each setup so the downfeed was kept to 1.5mm and crossfeed to 0.2mm. Not trying to race but need metal therapy after a of a week.
A turning tool grind was put on the tool and the load when cutting was minimal. I hope the pics show the surface finish achieved and even with a rough setup the overall size was acceptable. Within .002".
Butlers book on shaper work is a good starting point.
After lunch it's drilling and tapping.
BC
-
22nd Mar 2020, 09:59 AM #2Golden Member
- Join Date
- Dec 2007
- Location
- Adelaide
- Posts
- 575
I have always wanted a shaper but since we downsized just before I retired I no longer have the room - I'm envious.
-
22nd Mar 2020, 11:42 AM #3Most Valued Member
- Join Date
- Oct 2010
- Location
- melbourne, laverton
- Posts
- 1,910
Similar Threads
-
More shaper work and Clarkson grinder.
By steamloco1954 in forum METALWORK GENERALReplies: 4Last Post: 6th Dec 2019, 09:47 AM -
Shaper work 2. The tool holder
By steamloco1954 in forum METALWORK GENERALReplies: 3Last Post: 26th Nov 2019, 11:38 AM -
Shaper work
By steamloco1954 in forum METALWORK GENERALReplies: 5Last Post: 26th Nov 2019, 08:39 AM -
How to make a loco
By CGroves in forum METALWORK GENERALReplies: 4Last Post: 17th May 2014, 08:54 AM -
Old steam Loco on PM
By Ueee in forum METALWORK GENERALReplies: 1Last Post: 27th May 2012, 01:44 AM