Ratchet Cog's
Got asked by Sue's friend to replace 2 poorly made ratchet cogs off a table loom these had been made from old chopping board material one had lost 3 teeth.
20191207_103131.jpg
Got some 6061 bar stock
20200116_115704.jpg
Drew up new cogs with 18 teeth machine blanks to size. Each cog had a slight .5mm rise to keep the cog away from the frame of the loom so it will not ware or rub against.
20200120_101839.jpg
Made an arbour to mount the 2 cogs on simultaneously cutting each in opposite directions when mounted, the flat faces together. Using 60^ cutter at depth of 3mm x 10mm into the quadrant to form the ratchet.
Not bad for my first milling job, just need to double check everything in future is tight before & during.
20200204_122747[1].jpg20200204_163124.jpg20200212_105431.jpg20200213_101331.jpg20200214_120003.jpg
-
15th Feb 2020, 11:01 AM #2Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,943
Great work Ray. Only problem is that the part is so strong, what will she break next.
KrynTo grow old is mandatory, growing up is optional.
-
15th Feb 2020, 03:01 PM #3
Kryn she had not used it at all it was a recent acquisition and being an 8 shaft well worth the trouble to have a new one made. Besides the lady looks after me with sales to the spinners group and sometimes brings or send cakes home with Sue This job was $$ tho no cakes.
Similar Threads
-
Ratchet and Pawl source
By SurfinNev in forum METALWORK GENERALReplies: 10Last Post: 10th Dec 2019, 08:33 PM -
Douglas shaper ratchet
By Ueee in forum METALWORK GENERALReplies: 19Last Post: 19th Sep 2013, 12:23 PM -
Shaper table feed ratchet
By Ueee in forum METALWORK GENERALReplies: 10Last Post: 7th Jun 2012, 02:27 AM -
VICTORIA Powerbuilt Sockets, Ratchet, Breaker bar, 3/4"
By TermiMonster in forum METALWORK - Machinery, Equipment, MARKETReplies: 1Last Post: 6th May 2012, 09:14 PM