    Hi all,

    Since I have owned my mill it has not had a quill feed handle. So, after finishing the electrical and VFD parts I decided to make a quill feed handle. At first I was going to make one of the simple fixed handles where you need two hands to pull it out to the second detent to disengage the drive pin to re-adjust to another position, similar to one like this

    :https://www.ebay.com.au/itm/1X-Bridg...4AAOSwF25bJbN5

    But then I really liked the idea of a quick change lever like one of these:

    https://www.ebay.com.au/itm/Quill-Fe...EAAOxy4dNSrbNn

    It's much more usable in my opinion.

    So I decided to make my own, including the two pin engagement. I hunted the web high and low to get an idea of how these things are put together but details are light on, so I decided to design & make my own.

    The two pin positions were centre drilled and drilled using PCD calculations on an app on my phone. That method turned out to be very accurate indeed.

    I wanted a lever that had a generous amount of spring tension so that it had nice and positive engagement so I used a decent sized spring. This meant making the housing a little larger but I'm happy with the trade-off. I also screwd the top cover from underneath so that no additional screws can be seen - just an aesthetics thing I thought about.

    Overall it was a fair amount of mucking around in order to achieve a nice fit and feel but I got there in the end.

    Still yet to make a ball handle....

    Cheers,

    Simon
    Girl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.

  2. #2
    Join Date
    Dec 2013
    Age
    56
    Posts
    1,418

    Default

    Nice job Simon.
    Funny enough I've been looking at doing the same thing lately as it's been on the projects list for years. I've researched them several months ago, finding patents pictures etc again.
    Picture 1 of yours seems to be missing for me.

    I'm trying hard to finish me jib crane for this new garage, so I can get back into my few unfinished projects along with this handle.
    My 3 spoke handle always seems be in the way, even though I only have 1 of them in.
    Will be nice to reposition it.
    Using Tapatalk

  3. #3
    Join Date
    Aug 2011
    Location
    Melbourne
    Posts
    4,779

    Default

    Thanks Dave,

    I resubmitted the pics so hopefully it now works.

    I would be keen to see those patent drawings!

    Simon

    Sent from my SM-G970F using Tapatalk
    Girl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.

  4. #4
    Join Date
    Dec 2013
    Age
    56
    Posts
    1,418

    Default

    Here is the twin pin one. I didn't want to put my pictures up in case of copyright etc.
    https://patents.google.com/patent/US5267484A/en
    Using Tapatalk

  5. #5
    Join Date
    Aug 2011
    Location
    Melbourne
    Posts
    4,779

    Default

    Thanks Dave,

    That's useful information although a little late for me!

    That's a clever design, in some ways it's simpler than my design.

    Cheers,

    Simon

    Sent from my SM-G970F using Tapatalk
    Girl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.

Similar Threads

  1. Bridgeport clone quill power feed - required or not?
    By bollie7 in forum METALWORK GENERAL
    Replies: 16
    Last Post: 9th May 2019, 09:35 PM
  2. Handle of the cva quill.
    By welder in forum METALWORK GENERAL
    Replies: 0
    Last Post: 22nd Mar 2017, 05:02 PM
  3. WX#@%G AL-320G longitudinal/cross feed handle
    By burraboy in forum METALWORK GENERAL
    Replies: 6
    Last Post: 20th Mar 2015, 09:44 AM
  4. Drill press quill feed return spring fitment
    By Com_VC in forum METALWORK GENERAL
    Replies: 4
    Last Post: 2nd Jan 2014, 08:02 PM
  5. Bridgport clone power quill feed
    By BenM78 in forum METALWORK GENERAL
    Replies: 4
    Last Post: 23rd Jul 2010, 07:48 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •