Needs Pictures: 0
Results 1 to 15 of 102
-
20th Sep 2019, 03:28 PM #1Most Valued Member
- Join Date
- Aug 2011
- Location
- Melbourne
- Posts
- 4,779
Macson 18" Shaper spruce up WIP
Hi all,
I've had this shaper for a few years now and used it on several occasions however the wear on the ram and ways has prevented me from doing any work of reasonable tollerance.
So it's been sitting patiently in it's spot in the shed waiting for it's turn. While I have other projects on the go, I couldn't help but make a start since I have had my surface plate sitting and waiting.
I know for a fact that the ram and ways have considerable wear as does the dovetail gibb. First thing is to blue up the base of the ram and have a look;
Girl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.
-
20th Sep 2019, 03:36 PM #2Most Valued Member
- Join Date
- Aug 2011
- Location
- Melbourne
- Posts
- 4,779
The results of the first blue are not surprising. While there seems to be some smearing indicating too much blue but either way it's a sad picture. The eveness of my blue distribution and the quality of my scraping will hopefully improve as the cycles carry on. It's been a while since I did one of the Melbourne scraping classes so I'm playing catchup with my skills I acquired in that course.
At this stage I'm not too concerned with alignment to other planes or surfaces, I just want to start getting some increased contact. As the contact increases I will start to look at any variations in the width of the dovetail and squareness to the vertical ways etc. and then make some adjustments as required.
The second pic is after 6 cycles. a lot of work ahead of me!
Simon
Girl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.
-
20th Sep 2019, 05:48 PM #3Most Valued Member
- Join Date
- Aug 2011
- Location
- Melbourne
- Posts
- 4,779
Don't know what happened to the thread tittle!
Anyway. Results so far after 10 cycles. One side is getting alot more contact over the length. The other side is still playing catchup. There is a thin blue line just appearing on the outer edge of that side now as well.
I think I'm getting a little better with scraper blade control and consistency. I have played around with the tc scraper blade shapening angle. I initially sharpened to 6 degrees but have now changed to 5 degrees. Also the blue I am using is a home-brew made stuff using Shell alvania grease and prussian blue powder. I am finding it very difficult to spread over the larger area. I have scraped smaller items but the ram being the largest item I have scraped, I'm finding the blue to be too viscous to spread thinly. I think I will throw it in the microwave for 10 seconds and add a couple drops of oil to thin it down.
Also my shed is still too dusty. I have had a rather big cleanup in order to do this but still too dusty. I'm getting small foreign particles settle on the plate which is becomming annoying. I had also been having issues with the cleaning rag catching and leaving fibres on the inner edge of the bottom of the ram. I have since given that inner edge a light chamfer with a file to remove burs and casting imperfections which has helped.
I had forgotten how much like hard work this is! No wonder they invented biax machines!!!
Simon
Girl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.
-
20th Sep 2019, 07:40 PM #4
Big job with a hand scraper, but you will get there and look like Popeye when you're finished
Using Tapatalk
-
20th Sep 2019, 09:45 PM #5Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,945
-
20th Sep 2019, 09:55 PM #6Most Valued Member
- Join Date
- Aug 2011
- Location
- Melbourne
- Posts
- 4,779
While I haven't asked Joe if he wants to sell his biax, I'm tipping he will be hanging onto it. Even if it was for sale I doubt I could afford or justify the expense.
I'll press on bit at a time with my trusty hand scraper. It's quite liberating not not using power. Relaxing even.
Simon
Sent from my SM-G970F using TapatalkGirl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.
-
21st Sep 2019, 08:23 PM #7Most Valued Member
- Join Date
- Oct 2010
- Location
- melbourne, laverton
- Posts
- 1,910
nice
[QUOTE=simonl;1956834]Don't know what happened to the thread tittle!
Anyway. Results so far after 10 cycles. One side is getting alot more contact over the length. The other side is still playing catchup. There is a thin blue line just appearing on the outer edge of that side now as well.
I think I'm getting a little better with scraper blade control and consistency. I have played around with the tc scraper blade shapening angle. I initially sharpened to 6 degrees but have now changed to 5 degrees. Also the blue I am using is a home-brew made stuff using Shell alvania grease and prussian blue powder. I am finding it very difficult to spread over the larger area. I have scraped smaller items but the ram being the largest item I have scraped, I'm finding the blue to be too viscous to spread thinly. I think I will throw it in the microwave for 10 seconds and add a couple drops of oil to thin it down.
Also my shed is still too dusty. I have had a rather big cleanup in order to do this but still too dusty. I'm getting small foreign particles settle on the plate which is becomming annoying. I had also been having issues with the cleaning rag catching and leaving fibres on the inner edge of the bottom of the ram. I have since given that inner edge a light chamfer with a file to remove burs and casting imperfections which has helped.
I had forgotten how much like hard work this is! No wonder they invented biax machines!!!
Simon
im liking this thread all ready.
can you show us a photo of your marking out table(is that what you call it?)
does that mean you have to scrape the bottom half as well? how will you blue that bit?
aaron
-
21st Sep 2019, 08:44 PM #8Most Valued Member
- Join Date
- Aug 2011
- Location
- Melbourne
- Posts
- 4,779
Hi Aaron,
It's a granite surface plate.
I'll see if I can get out and take a pic tonight. Devastated by a magpie defeat atm so watching NRL prelim to take mind off it.
Once the base of the ram and dovetails are scraped flat and parallel, I then plan to blue up the ram to spot the machine base. Process starts again. The dovetails on the machine base will be interesting. Awkward scraping angle.
Somewhere along the line I also need to check alignment or squareness to vertical ways.
Simon
Sent from my SM-G970F using TapatalkGirl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.
-
21st Sep 2019, 08:52 PM #9Most Valued Member
- Join Date
- Aug 2011
- Location
- Melbourne
- Posts
- 4,779
I terms of scraping machines, I think a shaper is a good machine for a first attempt, especially one that has a fair bit of wear because I can't really make it any worse!
There's a lot to learn and a good portion of the learning comes from experience which I really don't have.
If i manage this project to my satisfaction then I'll have a crack at my mill.
Hopefully the membership on the forum can keep me progressing in the right direction.
Im certainly committed to scraping a couple of projects since I've spent the cash on the gear.
Simon
Sent from my SM-G970F using TapatalkGirl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.
-
21st Sep 2019, 09:17 PM #10
Where are you getting the cast iron stock to replace the gib? I'd like to know as I can only find round which is a waist for the price there asking for it.
Using Tapatalk
-
21st Sep 2019, 09:30 PM #11Most Valued Member
- Join Date
- Aug 2011
- Location
- Melbourne
- Posts
- 4,779
Hi Dave. I'm not looking to replace the Gibb. It's a parallel dovetail gibb not tapered and should still have plenty of meat left on it when I'm done.
Simon
Sent from my SM-G970F using TapatalkGirl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.
-
21st Sep 2019, 09:49 PM #12
Fair enough, I'm looking for a bit for my mill ram dovetail, I think the gib was dropped at factory and lost about 30-40mm from memory. Round is expensive if you have to turn most of it into chips.
Same with thick steel plates with large bores, I need to invest or make some trapanning tools.Using Tapatalk
-
21st Sep 2019, 10:36 PM #13Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,945
-
21st Sep 2019, 11:08 PM #14
Hi Kryn, a quick check 40mm would be perfect and it's about 400mm long, didn't look at thickness but probably around 10-12mm
Peter has spoken highly about you on your visit to Newcastle but we haven't met yet.
I'm about an hour out.Using Tapatalk
-
22nd Sep 2019, 01:12 AM #15Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,945
Hi Dave, I'll have a look tomorrow and see what I have around that size. He spoke of you also, next time I'm over that way I'll have to correct that issue, I'm sure Pete will help me on that?
Regards,
KrynTo grow old is mandatory, growing up is optional.
Similar Threads
-
Shaper, 18" Macson (Alba) shaper Brisbane
By pedro54 in forum METALWORK - Machinery, Equipment, MARKETReplies: 5Last Post: 9th Jul 2019, 12:02 PM -
Macson shaper gib adjustment
By Pete O in forum METALWORK GENERALReplies: 5Last Post: 10th Jul 2018, 11:54 PM -
Douglas 10" shaper
By Grahame Collins in forum METALWORK - Machinery, Equipment, MARKETReplies: 2Last Post: 26th Oct 2016, 10:31 AM -
Victoria Macson 18" metal shaper for sale
By Toggy in forum METALWORK - Machinery, Equipment, MARKETReplies: 7Last Post: 9th Jan 2016, 10:05 PM -
Macson 18" swing lathe
By Matt_M in forum EBAY, GUMTREE, and other off forum sales sitesReplies: 0Last Post: 13th May 2015, 09:59 AM