    The stop body is CI, the balance black steel and 1214.
    The body was originally a TAFE offcut of 75 x 75 mm extruded bar, squared in the lathe, bandsaw to divide.

    The adjustable stud is 12x1 mm thread with 20 mm length in contact.
    The graduations were done in the lathe fitted with spindle dividing plate and a triangular tip racked by the carriage - 10 divisions give 0.1 mm/div.
    One division is 3 adjacent strokes to mark one revolution (=1 mm).

    The setting block was made initially as accurately as possible, the body clamped in the vertical mill vise with the block and the prismatic surfaces fly-cut in the vertical mill.
    When tested, the angle was slightly large, measured with feeler gauges and one surface re-done with an appropriate packer on the setting block.

    The fiducial mark was a centre drill tip in the vertical mill.

    The stud nut is a bit of hex bar glued on, the nut some round bar with scallops on the vertical mill.

    John
    Attached Images Attached Images

Similar Threads

  1. Harrison M250 Cross-slide Dual Scale Problems
    By electrosteam in forum METALWORK GENERAL
    Replies: 7
    Last Post: 20th Apr 2021, 07:12 PM
  2. Harrison M250 Change Gear Test Spline
    By electrosteam in forum METALWORK PROJECTS
    Replies: 12
    Last Post: 16th Mar 2017, 11:45 AM
  3. Harrison M250 Metric Lathe - Imperial Screwcutting
    By electrosteam in forum METALWORK GENERAL
    Replies: 24
    Last Post: 17th Feb 2017, 06:20 PM
  4. Micrometer carriage 'stop'
    By Michael G in forum METALWORK PROJECTS
    Replies: 0
    Last Post: 10th Sep 2016, 04:59 PM
  5. Harrison M250 Turning Taper
    By electrosteam in forum METALWORK GENERAL
    Replies: 15
    Last Post: 7th Dec 2014, 04:07 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •