Needs Pictures: 0
Results 106 to 120 of 470
Thread: Brooks TC Grinder.
-
29th Aug 2019, 05:03 PM #106Most Valued Member
- Join Date
- Apr 2012
- Location
- Healesville
- Posts
- 2,129
G/day John, your drawings are very good.
I still use a pencil and ruler to draw my bits and pieces, I think next time my back goes out and I am marooned in a chair
I should have another crack at a drawing program.
cheers, shed
-
29th Aug 2019, 07:15 PM #107
Hi John,
Thanks for your post.
My personal recommendation for a draughting program would be "Qcad" primarily because its the one that I use. It runs on Linux, which is operating system that I use, also Windows and I believe Mac.
Basically its free ! Actually it has a 15 minute time period, after which it goes into a reduced function mode, but you can just save and restart to use all the functionality again. Most of which get little use. One of the functions I find most useful is its ability to save your drawing in a load of different image formats. It reads and writes DXF as well as DRW.
I've used dozens of 2D cad programs and this one for me is the very best. A perpetual licence costs £30 here and is well worth every penny.
It initially looks daunting but is very logical, plus you can click the help button or always ask me.Best Regards:
Baron J.
-
30th Aug 2019, 06:18 PM #108
Hi John, Guys,
I should have included this link to Ribbonsoft's Qcad.
https://www.ribbonsoft.com/en/
A little bit down the page is a link to the download page. Just choose which operating system you have and download the one you want. For people with CNC there is a version that outputs "G" code as well. I've never used that version.Best Regards:
Baron J.
-
5th Sep 2019, 10:01 PM #109Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 57
- Posts
- 2,672
Won't hijack your build, but just a quick note to say thanks for the QCad recommendation.
Checked it out and it felt reasonably intuitive so I bit the bullet a couple of nights ago and bought a license bundled with the "QCad Introduction to CAD" e-book.
My previous attempts at CAD have been a case of - I need to draw this so I'll try to do it using a CAD program -followed by the inevitable frustration and tossing it over my shoulder.
Have decided to give it a decent crack and see if I can break through that point where you give up because its quicker/easier to draw it by hand. Trying to spend at least half an hour an evening working through the concepts and exercises in the e-book and see where it ends up. Only up to chapter 6 so far, but it feels like its sinking in, so fingers crossed
Steve
-
8th Sep 2019, 02:06 AM #110
Hi Steve,
I'm pleased that you have obtained a copy of Qcad, ! It is like anything else it takes a little while to get into it.
I've done many drawings using it. I also use the print feature to produce a working copy of things that I'm making, and of course to post on the forum.
I must confess that I didn't buy the book, however I do use the help file now and again, usually to remind me about little used commands.
If I can help in any way please don't hesitate to ask me.Best Regards:
Baron J.
-
9th Sep 2019, 11:36 PM #111
Topslide machining.
Hi Guys,
I've machined the topslide to create a channel for the leadscrew assembly to run in. Its a simple 10 by 10 mm slot the full length of the topslide. The actual slot width is not at all critical as is the depth, since I intend to use an M8 threaded bar for the leadscrew and support it at either end in brass bearings. They will of course have to be fitted to suit the slot.
01-09-2019-001.jpg 09-09-2019-013.jpg 01-09-2019-002.jpg
I machined the slot in two 5 mm deep passes. That last picture was taken after the first pass. The piece of square tool steel was to make sure that the chuck cleared the edge of the machine vise.
I've now to drill the holes to fasten the leadscrew supports and make them.
Thanks for looking.Best Regards:
Baron J.
-
13th Sep 2019, 06:24 AM #112
More top slide work.
Hi Guys,
Many thanks to those forum members that are still with me on this project !
After the motor problems with the mill, things got a bit out of shape. Anyway I've managed to finish the slot in the bottom of the topslide, drilled the holes for the leadscrew support bearings.
I've actually cut the slot to 12 mm wide because of the rough surface finish caused by a damaged cutter Its still 10.25 mm deep, just a little wider than drawn.
12-09-2019-001.jpg
In order to ensure that I had the holes exactly in the centre of the slot, I made a gauge pin that fitted the pilot holes
12-09-2019-003.jpg 12-09-2019-002.JPG
The idea being that I could use feeler gauges to determine the gap between the sides and the gauge pin and then I would know how far off the centre line I was and I could take another cut off one side or the other if needed.
12-09-2019-005.JPG 12-09-2019-004.JPG
As it happens, whilst I could just see light from one side, I couldn't slide a 1 thou feeler gauge between the gauge and slot wall. The other end was such that I couldn't see any light getting between them at all.
After I drilled and reamed the two holes in the ends of the topslide to 8 mm and then deburred them.
12-09-2019-006.jpg
I picked up a couple of pieces of scrap brass bar from the scrapyard. The thicker piece is only just long enough to get both ends out of. Its 42 mm long. I propose to turn each end down to 8 mm for a distance of ten mm. Drill right through 4.2 mm and tap the hole M5 from both ends, and then part the piece in half.
Thanks for looking.Best Regards:
Baron J.
-
13th Sep 2019, 10:56 PM #113
Brass bearings.
Hi Guys,
I've now turned some brass bits to make the bearings for the top slide lead screw supports.
13-09-2019001.jpg 13-09-2019002.jpg 13-09-2019003.jpg
In this first picture they have been placed in the holes intended for them. They need flats machining on them so that they will fit into the channel in the top slide. There are supposed to be three bearing support bushes, but I need to get another piece of brass bar to make what will become the nut that the leadscrew runs in and uses to pull the top slide back and forth.Best Regards:
Baron J.
-
15th Sep 2019, 05:36 AM #114
Leadscew support bearings.
Hi Guys,
After sorting out the difficulties with machining the sides of the bearings that fit into the channel that I've machined in the bottom of the TCG top slide, I'm now ready to make the leadscrew. So that will be the next job.
14-09-2019=011.jpg
This is a family picture of all the current parts for the leadscrew, which has yet to have the ends machined to fit the bearings. Also a nut has yet to be made that runs on the leadscrew and drives the table.
13-09-2019008.jpg 13-09-2019007.jpg
This is one of the bearings showing how it would be placed when the leadscrew is fitted. The bearing in this picture is the one that I turned off the body, to make a 8 mm X 20 mm long support for holding the rather short stub in an 8 mm collet to prevent it slipping.
14-09-2019=007.JPG 14-09-2019=012.JPG
This first picture is one of the bearings before having the hole for the end of the leadscrew drilled in it. The other is the finished bearings complete with the M6 Allen hex countersunk screws.
14-09-2019=004.JPG 14-09-2019=010.JPG
You will notice that they have had 2 mm diameter holes drilled through them. This is so lubrication can easily be provided to the bearings at each end. Hopefully the lubrication will find its way onto the leadscrew as well.
As you can see, I just used an M6 threading die gripped in the drill vise to support the screw whilst drilling.
14-09-2019=008.JPG 14-09-2019=009.jpg
The holes in each end of the top slide were countersunk to take the screw heads. The hex socket providing a small oil well for the lubricating oil.
My thanks to all, especially those nice people who helped me with advice and support with getting my bearing machining problem sorted out.Best Regards:
Baron J.
-
15th Sep 2019, 08:05 AM #115Most Valued Member
- Join Date
- Sep 2011
- Location
- Ballarat
- Age
- 65
- Posts
- 3,103
Still watching and still loving this thread John. I'm also getting some great tips and tricks I can use.
Keep up the great work.
Phil
-
15th Sep 2019, 07:51 PM #116
Hi John,
Well you might not think that the length of bright rolled bar that I used for the top slide would move
Well it has, the top of the slot has opened out around 1.5 thou along the whole length of the bar ! I can no longer get it to fit into the saddle. I must admit that I became suspicious when I came to fit the brass bearings. They fitted perfectly at the top of the slot and I had to file them slightly to get them to drop to the bottom of the slot.
I wish I had a horizontal grinder ! I don't think that trying to machine a thou or so off one edge is going to be easy. Ah well, you can't win them all.Best Regards:
Baron J.
-
15th Sep 2019, 08:04 PM #117Golden Member
- Join Date
- Nov 2010
- Location
- Gippsland Victoria
- Posts
- 733
Would it be possible to mount a dremel grinding point or wrap some emery paper around a rod in the lathe chuck and with the workpece mounted on an angle plate slowly wind the workpiece past the tool ?
I havent got a clue if that would work or not but it may spark other thoughts.
Bill
-
15th Sep 2019, 09:29 PM #118
Hi Bill,
Thanks for your suggestion !
This is a difficult one. I need to get not only the top edge of the outside reduced but inside the top edge of the slot where the bearings run. There isn't a lot to play with there.
I've spent hours fitting the top slide so there was minimal side and end play on there.
I suppose that I can blame poor planning ! In hindsight I could have machined the "T" slot and the leadscrew channel first and then cut the slots in the sides for the support bearings to run in. Taking an original design and stamping your own concept on it is not as easy as I thought !
I think grinding would be the way to go. I suspect that I'm going to have to start scraping to get the slot clearances back. I need to think about this some more.Best Regards:
Baron J.
-
18th Sep 2019, 06:17 AM #119
Fitting the brass bearings !
Hi Guys,
Among other things I've spent some time fitting the brass bearings for the leadscrew and turning the leadscrew ends to size. I just need to make a knob to turn the leadscrew and finish refitting the topslide so that it moves smoothly without binding. I've also found a small lump of bronze that I'm going to use to make the nut that the leadscrew uses to move the topslide.
17-09-2019-01.jpg 17-09-2019-03.JPG 17-09-2019-02.jpg
These two pictures shown from underneath the completed topslide with the leadscrew fitted into its bearings. The third one is a view from the top showing the fixing screws securing those bearings.
17-09-2019-04.jpg 17-09-2019-05.jpg
These last two pictures are just family ones of the finished bits that were used.
Top Slide 3b .png
This drawing is that of the brass bearings.
That is all so far, I've been spending a great deal of my time making the stand for the 6X4 bandsaw. I hope to get it finished and ready for painting by the weekend.
Thanks guys.Best Regards:
Baron J.
-
23rd Sep 2019, 04:35 AM #120
Leadscrew nut !
Hi Guys,
While waiting for the paint to dry on the bandsaw stand, I've been machining a bit of bronze bar to make a nut to fit on the leadscrew of the TCG. The sides were fly cut on the mill and the spigot turned using the four jaw on the lathe. That spigot is 8 mm in diameter and is intended to drop into a hole drilled in the saddle with an M6 countersunk screw to secure it. I've still that bit to do along with a knob for the end of the leadscrew.
22-09-2019-004.JPG 22-09-2019-005.JPG
Its turned out quite well. Its threaded M8 to suit the leadscrew and M6 for the fastening screw.
22-09-2019-007.JPG 22-09-2019-006.JPG
I did make a small boo boo I hadn’t realised that I was cutting deeper and deeper until I hit the tops of the threads ! Of course by then it was too late. The thickness at the outer edges is spot on but its about a mm deeper in the centre. I just hope that it hasn't weakened the spigot too much.
Thanks for looking guys.Best Regards:
Baron J.
Similar Threads
-
Hercus tool and cutter grinder & cylindrical grinder.
By stix012 in forum EBAY, GUMTREE, and other off forum sales sitesReplies: 1Last Post: 23rd Aug 2018, 05:31 PM -
Heald internal grinder & Heald Planetary grinder
By achjimmy in forum METALWORK - Machinery, Equipment, MARKETReplies: 2Last Post: 11th Oct 2017, 09:22 PM -
New to me old grinder.
By DSEL74 in forum ANTIQUE AND VINTAGE MACHINERYReplies: 12Last Post: 30th Sep 2016, 08:35 PM -
Roller grinder ways/ plain grinder ways
By Michael G in forum METALWORK GENERALReplies: 11Last Post: 6th May 2012, 12:37 AM -
Anyone used this Grinder?
By bwal74 in forum METALWORK GENERALReplies: 6Last Post: 10th Apr 2012, 07:47 PM