    Default tap wrench

    I asked about making one of these sometime back...thought it was time that I got off my backside and did something about it

    I am happy with the way it turned out.
    MrPete222 tip 393 video helped me out the calcs for milling the slot...worked a treat
    20190131_115053[1].jpg20190131_115059[1].jpg

  2. #2
    Join Date
    Oct 2010
    Location
    NSW
    Posts
    181

    Default

    Nice one.

  3. #3
    Join Date
    Aug 2011
    Location
    Melbourne
    Posts
    4,779

    Default

    Good work. Nice knurling too.

    Simon
    Girl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.

  4. #4
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,477

    Default

    Hi Eskimo,

    Very nicely done ! I've not seen one made quite like that.
    I do agree with Simon, the knurling looks really good, a nice sharp pattern.
    Best Regards:
    Baron J.

  5. #5
    Join Date
    Jul 2006
    Location
    Athelstone, SA 5076
    Posts
    4,258

    Default

    Quote Originally Posted by BaronJ View Post
    Hi Eskimo,

    Very nicely done ! I've not seen one made quite like that.
    I do agree with Simon, the knurling looks really good, a nice sharp pattern.
    Yeah...the knurling surprised me too

    Thanks Simon and Baron

    I copied "This old Tony"'s tap wrench...you tube it.

  6. #6
    Join Date
    Jun 2013
    Location
    Tasmania
    Posts
    257

    Default

    Lovely work.

    What material did you use?

    I really need to consider making one, or buying a decent wrench. I've broken and cracked the cheap crappy ones I've had and they hold terribly and are made from cheese.

    Thanks.

  7. #7
    Join Date
    Jul 2006
    Location
    Athelstone, SA 5076
    Posts
    4,258

    Default

    Quote Originally Posted by Hornetb View Post
    Lovely work.

    What material did you use?

    I really need to consider making one, or buying a decent wrench. I've broken and cracked the cheap crappy ones I've had and they hold terribly and are made from cheese.

    Thanks.

    Handles were BMS but the jaws was from stuff a mate gave from his toolmaking days a few years ago...so I am guessing/hoping it might be good stuff so I can harden them?

  8. #8
    Join Date
    Nov 2004
    Location
    Bungama SA
    Age
    52
    Posts
    960

    Default

    As soon as I seen your picture I thought of This old Tony
    ....................................................................

  9. #9
    Join Date
    Jul 2006
    Location
    Athelstone, SA 5076
    Posts
    4,258

    Default

    And another...this time my version of a starret 174
    20190207_100743.jpg
    20190207_100824.jpg20190207_100828.jpg
    20190207_175304.jpg

    Yes you can see the end mill marks...but I intend to harden and grit blast and parkerise...so hopefully they should disappear....with a bit of luck
    Attached Images Attached Images

  10. #10
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,477

    Default

    Hi Eskimo,

    Looks good ! Should be even nicer when you have treated it.

    I have a Starret one, its many years old. I keep meaning to remove the screw and put a hardened tip on it. Mine has mushroomed badly and will need to be filed to get the screw out. Another round toit I'm afraid, its somewhere in there
    Best Regards:
    Baron J.

  11. #11
    Join Date
    Jul 2006
    Location
    Athelstone, SA 5076
    Posts
    4,258

    Default

    Quote Originally Posted by BaronJ View Post
    Hi Eskimo,

    Looks good ! Should be even nicer when you have treated it.

    I have a Starret one, its many years old. I keep meaning to remove the screw and put a hardened tip on it. Mine has mushroomed badly and will need to be filed to get the screw out. Another round toit I'm afraid, its somewhere in there
    I had a small hardened dowl that I used

  12. #12
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,477

    Default

    Hi Eskimo,

    Yes I really ought to pull it out of its hiding place and do something like that. I do think that its a weakness of this type of tap wrench. I used to have one that came in a box of taps & dies, the screw handle was made from monkey metal and broke off the first time I used it. I sawed it in half to release the tap before throwing it in the scrap bin.

    I currently use a similar one with a sliding "V" block.
    Best Regards:
    Baron J.

  13. #13
    Join Date
    Jul 2006
    Location
    Athelstone, SA 5076
    Posts
    4,258

    Default

    My version of the Starret
    20190227_120603.jpg

    Not finished ....have to do plunger and spring and bore and cut V in centre bit...etc

  14. #14
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,477

    Default

    Hi Eskimo,

    That looks posh even unfinished I'm going to have to keep an eye on this one
    Best Regards:
    Baron J.

  15. #15
    Join Date
    Jul 2006
    Location
    Athelstone, SA 5076
    Posts
    4,258

    Default

    wonder what the plungers cost?..wondering if I should buy one in lieu of making one...If I buy I wont have to harden it

    would silver steel be okay to make the plunger and harden and temper afterwards?

    edit: they are US$6.22 each for this size...but will it fit?...as I have no idea if I am any where close to their dimensions..I just took a good picture form the web and expanded its size till it was about 9 inches in length...what I got is what I have shown.

Page 1 of 2 12 LastLast

Similar Threads

  1. DIY Tap wrench
    By eskimo in forum METALWORK GENERAL
    Replies: 24
    Last Post: 31st Aug 2018, 06:37 PM
  2. Collet Nut Wrench
    By BaronJ in forum METALWORK GENERAL
    Replies: 3
    Last Post: 28th Aug 2015, 11:17 PM
  3. HIT Piipe wrench
    By WesP in forum METALWORK GENERAL
    Replies: 6
    Last Post: 24th Feb 2014, 09:09 PM
  4. Open end wrench as a caliper.
    By aametalmaster in forum METALWORK GENERAL
    Replies: 7
    Last Post: 9th May 2012, 12:39 AM
  5. Impact Wrench
    By electrosteam in forum METALWORK GENERAL
    Replies: 9
    Last Post: 27th Jul 2010, 11:52 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •