I will ask again.
Would silver steel be suitable for the plunger. I would home harden and temper!
-
1st Mar 2019, 10:04 PM #17Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,959
Nice work and yes, that should be fine, at least it won't mushroom on you.
KrynTo grow old is mandatory, growing up is optional.
Similar Threads
-
DIY Tap wrench
By eskimo in forum METALWORK GENERALReplies: 24Last Post: 31st Aug 2018, 06:37 PM -
Collet Nut Wrench
By BaronJ in forum METALWORK GENERALReplies: 3Last Post: 28th Aug 2015, 11:17 PM -
HIT Piipe wrench
By WesP in forum METALWORK GENERALReplies: 6Last Post: 24th Feb 2014, 09:09 PM -
Open end wrench as a caliper.
By aametalmaster in forum METALWORK GENERALReplies: 7Last Post: 9th May 2012, 12:39 AM -
Impact Wrench
By electrosteam in forum METALWORK GENERALReplies: 9Last Post: 27th Jul 2010, 11:52 PM