    Hi Guys,

    I think that I would have extended the sealing strip to go right around that lip. You have effectively created a gap above where coolant can get between the two lips above the strip and run between them.

    A trick that I've done in the past to create a seal when I didn't have a suitable gasket was to use hot melt adhesive !

    The application at the time was a washing machine water pump. It had a cast monkey metal support for the motor and a Bakelite cover that was held on by three spring clips round the edge. I greased the pump cover edges and heated the casting with a cooks torch, then ran a bead of hot melt around where the gasket would have been. I fastened the two parts together whilst still hot and trimmed the flash off with a Stanley knife when it had cooled.

    The grease stopped the hot melt from sticking to the cover and allowed it to be removed without disturbing the hot melt. That pump was still in use nearly eight or nine years later without leaking when it got scrapped due to drum failure.

    I still have the replacement seal for the pump, but it was never fitted. I also still have the motor and controller from the washer ! Waiting to be used for something or other useful.
    Best Regards:
    Baron J.

  2. #32
    Join Date
    Apr 2012
    Location
    Healesville
    Posts
    2,129

    Default

    Quote Originally Posted by BaronJ View Post
    Hi Guys,
    I think that I would have extended the sealing strip to go right around that lip. You have effectively created a gap above where coolant can get between the two lips above the strip and run between them.
    Hi John, I had a pretty good look where it was and wasn't leaking and it is not leaking now so i will just keep an eye on it, the clamp
    and the seal seems to have done the trick and if it does leak again i will have another go at it.

    I think the coolant is pretty much flung off the wheel before it gets to the second baffle.

    Here is a pic showing how churchill has dealt with returning the coolant from the wheel guard.

    cheers, shed
    Attached Images Attached Images

  3. #33
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,480

    Default

    Thanks John,

    I had no idea that there were baffles in there ! Your picture helped make it clear to me why you only put the sealing strip where you did.

    Looking good I'm watching and learning
    Best Regards:
    Baron J.

  4. #34
    Join Date
    Apr 2012
    Location
    Healesville
    Posts
    2,129

    Default Adjustment and measurement

    I wanted a better/quicker and accurate way to adjust the table and also a way to accurately know how much I am grinding (DOC) and more accurate finishing so I have added a couple of indicators.

    The Syvac, I fitted a rubber dust boot to the plunger and I bored a bit of aluminum and slid it on the other end to protect the outer end of the plunger.
    The mounting bracket is made out of 50mm SHS and clamps on to the cast iron splash tray, the indicator is fitted to a spring loaded swing away mounting and this also has a micro switch that retracts the grinding head almost instantaneously should the adjustable rod give it a shove in a moment of brain fade on my behalf.
    I thought that the indicator reading would bounce around a bit when the machine was running but it gives a very steady reading.

    The adjustable rod is adjusted to suit the diameter of the job to be ground and also has enough length to accommodate for wheel wear and new full dia wheels.
    For an anvil it has a short length of HHS pressed into a bored hole in the end of the rod and then ground to finish it.

    The adjustable arm and the indicators for checking the job and adjusting the table are removed after use and put away before grinding.

    cheers, shed
    Attached Images Attached Images

  5. #35
    Join Date
    Oct 2008
    Location
    N.W.Tasmania
    Posts
    1,407

    Default

    That looks really nice Shed, well thought out and nicely executed. Like John (Barron) I am watching and learning too.

Page 3 of 3 FirstFirst 123

Similar Threads

  1. Churchill Cylindrical Grinder. Free to good home.
    By Machtool in forum METALWORK - Machinery, Equipment, MARKET
    Replies: 15
    Last Post: 8th Sep 2016, 12:21 AM
  2. No9 Cylindrical Grinder
    By neddyo in forum THE HERCUS AREA
    Replies: 8
    Last Post: 27th Aug 2015, 08:19 AM
  3. Churchill slideway grinder
    By markgray in forum EBAY, GUMTREE, and other off forum sales sites
    Replies: 0
    Last Post: 17th Jun 2014, 06:41 PM
  4. Transporting Churchill surface grinder
    By bob ward in forum METALWORK GENERAL
    Replies: 9
    Last Post: 22nd May 2014, 05:30 AM
  5. Churchill Surface Grinder handbook request
    By Abratool in forum METALWORK GENERAL
    Replies: 8
    Last Post: 11th May 2012, 11:11 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •