OK more Rotary Engine projects. I got a couple of these OMC Rotary Engines, these engine were use in the Evinrude & Johnson Snowmobiles back in 1974, these two are the 45 hp versions there is a 35 hp version as well. This project has not started out well I took apart the first engine as you can see the housing is severely damaged I'm not a happy man at the moment
Resize of IMG_7241.jpgResize of IMG_7258.jpgResize of IMG_7263.jpg
-
20th May 2019, 08:48 PM #2
The auxiliary air valve is a fatal flaw on these engines, if not remove this is what happens. I finish off the tear down of the engine and clean up the main parts of the engine, the side plates are in good cond so is the E shaft and the rotor. One thing i notice on the rotor there is a blind rivet, is that rivet meant to stop the bearing from slipping out ? I think i will replace the rotor bearing as well and replace the apex seals. and housing.
Resize of IMG_7261.jpgResize of IMG_7270.jpgResize of IMG_7269.jpgResize of IMG_7276.jpg
-
20th May 2019, 08:53 PM #3
I clean up the housing so i can get a better look at the damage
Resize of IMG_7283.jpgResize of IMG_7279.jpgResize of IMG_7278.jpg
-
20th May 2019, 10:05 PM #4Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,559
Ouch - that's not nice. Can it be welded up or will that warp everything to buggery?
Michael
-
20th May 2019, 11:52 PM #5
No not nice,but that's why it was cheap. No can't weld it to much work and need to strip off the special coating and re coat it and machine it to the right profile and could warp everything. I place a order for a new housing from Freedom Motors
-
21st May 2019, 06:15 AM #6
I clean up the rotor and cooling fan components. The fan housings have a few cracks in them, the rotor is in good shape. The charge coils are crack, new ones are on the way.
Resize of IMG_74.jpgResize of IMG_7274.jpgResize of IMG_7273.jpgResize of IMG_7296.jpgResize of IMG_7294.jpgResize of IMG_7295.jpg
-
21st May 2019, 09:34 PM #7
Got a couple of new parts. New housing and new corner seals and springs and new Stator.
Resize of IMG_7316.jpgResize of IMG_7312.jpgResize of IMG_7313.jpgResize of IMG_7314.jpgs-l1600.jpg
-
21st May 2019, 09:46 PM #8
Been going through the Electrical system, the new Stator i can not use only the charge coils. The power pack, starter solenoid looks to be ok but the ignition coil is toast So on the look out for a new one. I have notice a lot of coils to suit OMC Johnson Evinrude Outboard Marine motors
Resize of IMG_71.jpgResize of IMG_7319.jpgResize of IMG_7298.jpgResize of IMG_7323.jpg
-
22nd Jun 2019, 02:40 PM #9
I drilled and tap a 1/8 pipe thread to seal off the valve
Resize of IMG_7448.jpgResize of IMG_7449.jpgResize of IMG_7451.jpgResize of IMG_7450.jpg
-
22nd Jun 2019, 02:45 PM #10
I decided to pull apart the second OMC engine. This engine has been sitting for a very long time, all the seals are stuck so will give a good soak for a while. As you can see in the photos of the rotor there is a blind rivet and also a pin in the bearing race cup, so looks like these engines have the blind rivet and pin to hold the bearing in situ.
Resize of IMG_7457.jpgResize of IMG_7458.jpgResize of IMG_7459.jpgResize of IMG_7460.jpgResize of IMG_7461.jpgResize of IMG_7462.jpgResize of IMG_7463.jpg
-
22nd Jun 2019, 02:50 PM #11
The housing and side plates are in good cond, there is a small chip inside the housing surface . The chip is near the intake side so may be ok for running as is me thinks.
Resize of IMG_7467.jpgResize of IMG_7468.jpgResize of IMG_7466.jpgResize of IMG_7469.jpg
-
22nd Jun 2019, 03:25 PM #12Most Valued Member
- Join Date
- Jul 2016
- Location
- Melbourne
- Age
- 35
- Posts
- 1,522
What is the chip caused by do you think, detonation?
Great seeing the detail on these small rotaries keep it up.
-
22nd Jun 2019, 04:46 PM #13
-
5th Aug 2019, 03:25 PM #14
I finally got most of the new parts from the US to start the rebuild. I can now start rebuilding the first engine, also been experimenting on machining up a adapter flange for the E crank shaft seal. i can get seals here in AUS for $5 The original seals are $55 USD. I'll see if i can find a smaller OD on the seal, like to have a bit more material on the bore.
IMG_7535.jpgResize of IMG_7505.jpgResize of IMG_7501.jpgResize of IMG_7502.jpgResize of IMG_7503.jpgResize of IMG_7504.jpg
-
7th Aug 2019, 04:41 PM #15
Been busy cleaning all the parts before i start the rebuild. I decided to lap the end plates on my surface plate with 800 grit wet and dry sandpaper.
Resize of IMG_7506.jpgResize of IMG_7507.jpgResize of IMG_7509.jpgResize of IMG_7508.jpg
Similar Threads
-
Windsor engine
By azzrock in forum AUTO PARTS / Wanted, For Sale - HELPReplies: 21Last Post: 2nd Jan 2021, 06:46 PM -
Goggo Engine
By Goggomobile in forum AUTO RESTORATIONReplies: 0Last Post: 1st Jul 2016, 09:03 PM -
Stirling engine help
By xXvapourXx in forum METALWORK GENERALReplies: 14Last Post: 9th Jul 2011, 11:35 AM