    Finish the top coat on the main body of the mill. I had a problem when rolling out the final coat, the foam roller was leaving small air bubbles on some of the areas on the mill. so i gave it a light sanding with 800 grit sandpaper and use some fine automotive cut and polish.

    Resize of IMG_6620.jpgResize of IMG_6617.jpgResize of IMG_6619.jpg

  2. #17
    Join Date
    Oct 2016
    Location
    Melbourne
    Posts
    224

    Default



    Done the first coat of primer on the knee. Went out and got one of those airless spray guns, WOW it did the job really well and took me 5 minutes to paint. I will get most of the parts degrease and prep for painting.

    Resize of IMG_6611.jpgResize of IMG_6616.jpgResize of IMG_6612.jpgResize of IMG_6613.jpgResize of IMG_6614.jpgResize of IMG_6615.jpg

  3. #18
    Join Date
    Oct 2016
    Location
    Melbourne
    Posts
    224

    Default

    I finally got the knee painted and the other parts and fitted back on the main body of the mill, i replace the two thrust bearings with new ones and found the shaft is bent will machine a new one once the mill is up and running. I'll get some new Flush Grease Zerk Nipple Fittings as i can not push oil through some of them. Next is cleaning and panting the drive motor and saddle and gearbox.


    Resize of IMG_6628.jpgResize of IMG_6629.jpgResize of IMG_6630.jpgResize of IMG_6631.jpgResize of IMG_6632.jpgResize of IMG_6633.jpg

  4. #19
    Join Date
    Oct 2016
    Location
    Melbourne
    Posts
    224

    Default

    Work on the mill is progressing nicely no major problems at this stage. Have got another batch of parts painted in primer undercoat. Took the front cover off the gearbox and gave it a good clean inside, all the gears are in good shape and the shifting mechanism is in good shape as well, no cracks in the plastic parts.

    Resize of IMG_6640.jpgResize of IMG_6638.jpgResize of IMG_6639.jpgResize of IMG_6642.jpgResize of IMG_6641.jpgResize of IMG_20180430_133706.jpgResize of IMG_20180430_133847.jpgResize of IMG_20180430_133858.jpgResize of IMG_6634.jpgResize of IMG_6636.jpg

  5. #20
    Join Date
    Oct 2016
    Location
    Melbourne
    Posts
    224

    Default

    OK gearbox and saddle are back on the mill, replace the thrust bearings the bearings in the gearbox are in good shape. Have some more parts that will need repairing or replace that will be in the next lot of photos.

    Resize of IMG_6650.jpgResize of IMG_6648.jpgResize of IMG_6649.jpg

  6. #21
    Join Date
    Oct 2016
    Location
    Melbourne
    Posts
    224

    Default

    Stated cleaning the ram and rack and pinion gear, there some teeth missing on the rack and the pinion gear is in bad shape. Does anyone know were there is any general engineering services here in Melbourne that could help me out with getting this part fix

    Resize of IMG_6656.jpgResize of IMG_6661.jpgResize of IMG_6657.jpgResize of IMG_6659.jpgResize of IMG_6658.jpgResize of IMG_6660.jpg

  7. #22
    Join Date
    Oct 2016
    Location
    Melbourne
    Posts
    224

  8. #23
    Join Date
    Oct 2016
    Location
    Melbourne
    Posts
    224

    Default

    Today it's been cold and wet no good for painting parts, so started work on the head. I wont do a complete tear down no need for it the bearings feel and sound in good shape, i may replace the taper bearings. I will need to make up a new part which i think it's made out of copper. Now as you can see the photo of the small gearbox it has some old grease. I'm a bit confused do i reapply grease the manual does not say anything about grease, just add oil on top of the spindle and there is a oil port on the side of the quill housing.

    Resize of IMG_6685.jpgResize of IMG_6686.jpgResize of IMG_6687.jpgResize of IMG_6688.jpgResize of IMG_6690.jpgResize of IMG_6702.jpgResize of IMG_6689.jpgResize of IMG_6699.jpgResize of IMG_6698.jpgResize of IMG_6697.jpgResize of IMG_6700.jpg

  9. #24
    Join Date
    Oct 2016
    Location
    Melbourne
    Posts
    224

    Default

    I remove a few more parts off the head today and gave it a good clean. I have come to a conclusion that the down feed gear box is oil lubricated, this head has been work on before.

    Resize of IMG_6712.jpgResize of IMG_6715.jpgResize of IMG_6718.jpgResize of IMG_6716.jpgResize of IMG_6717.jpgResize of IMG_6723.jpgResize of IMG_6719.jpgResize of IMG_6720.jpgResize of IMG_6722.jpg

  10. #25
    Join Date
    Sep 2016
    Location
    Morphett Vale SA
    Age
    52
    Posts
    21

    Default

    Very nice work and thanks for taking the time to document the process.Could you please detail the brands of primer,filler and paint you are using?
    Thanks in advance,Nick

  11. #26
    Join Date
    Oct 2016
    Location
    Melbourne
    Posts
    224

    Default

    G'day Nick,
    Thanks mate. I'm using dulux metal shield primer and top coat paint. No filler. http://www.duluxprotectivecoatings.c...o-Brochure.pdf

    Cheers,
    Mark.
    Quote Originally Posted by rustyovali View Post
    Very nice work and thanks for taking the time to document the process.Could you please detail the brands of primer,filler and paint you are using?
    Thanks in advance,Nick

  12. #27
    Join Date
    Oct 2016
    Location
    Melbourne
    Posts
    224

    Default

    I fix the lever for the drive feed gearbox, as you can see the original DETENT SPRING was in pieces so fitted a SPEED GEAR DETENT BALL AND SPRING set, had to shorten the spring but now the lever stays in the stop position.

    Resize of IMG_6645.jpgResize of IMG_6670.jpgResize of IMG_6671.jpgResize of IMG_6672.jpg

  13. #28
    Join Date
    Oct 2016
    Location
    Melbourne
    Posts
    224

    Default



    I had a couple of parts that need to be fix by a local engineering workshop, the feed drive electric motor armature was in bad shape and the spindle drive motor base plate had a crack in it so they are getting repaired.

    Resize of IMG_6664.jpgResize of IMG_6663.jpg

  14. #29
    Join Date
    Oct 2016
    Location
    Melbourne
    Posts
    224

    Default

    Almost finish painting the mill head, got new tapped bearings and have found some issues to address with the head, will go through with this when putting it back together

    Resize of IMG_6726.jpgResize of IMG_6727.jpgResize of IMG_6728.jpgResize of IMG_6730.jpgResize of IMG_6729.jpg

  15. #30
    Join Date
    Oct 2016
    Location
    Melbourne
    Posts
    224

    Default

    The ram is painted, but need to replace the spur gear which is on order will machine the old gear off and weld the new gear on. Been looking around to get a couple of new metal nameplates made up, so i got a price of $700 for the two

    Resize of IMG_6734.jpgResize of IMG_6733.jpgResize of IMG_20180603_061345.jpg



Page 2 of 4 FirstFirst 1234 LastLast

Similar Threads

  1. Okuma LP Lathe Clean Up and Repair
    By Turbine Builder in forum ANTIQUE AND VINTAGE MACHINERY
    Replies: 49
    Last Post: 4th May 2017, 06:41 PM
  2. Replies: 2
    Last Post: 17th Apr 2017, 07:29 PM
  3. Clean Metal
    By YarrD in forum METALWORK GENERAL
    Replies: 46
    Last Post: 3rd Apr 2011, 04:01 PM
  4. Rambaudi Mill Information
    By dreinoga in forum METALWORK GENERAL
    Replies: 3
    Last Post: 2nd Mar 2011, 10:25 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •