    Default Cloth insulation tape.

    A while back I made two wiring harnesses, one for ignition, the other for lights. I wrapped both up in plastic insulation tape, not an easy job keeping the cables straight and in the same order for the harness length. I managed that reasonably well, but after wrapping the harnesses were s tiff as a board and twisted.

    This morning some cloth insulation tape arrived, so I cut the old plastic stuff off and wrapped both harnesses in the cloth tape, boy what a difference. The harnesses are now quite straight, pliable and easier to thread through the frame. Big improvement. Good stuff this cloth insulation tape.

    Tomorrow I'll solder on some more terminals for the rear end, shorten a couple of leads and hook everything up.

    The tape had to come from China of course, couldn't find and suppliers in Oz. So many things you just can't buy in Australia, Go down the street to buy cable, terminals, bearings and so on, visit half a dozen shops and come home empty handed. No
    wonder everyone is turning to online shopping, usually from overseas sellers.
    Attached Images Attached Images

  2. #2
    Join Date
    May 2020
    Location
    Willowbank QLD
    Posts
    535

    Default

    I was looking for cloth tape today and saw your post. Which supplier did you get it through. It saves a lot of stress knowing you had good results as there are heaps to choose from.

    Thanks Steve

  3. #3
    Join Date
    May 2020
    Location
    Willowbank QLD
    Posts
    535

    Default

    I was looking for cloth tape today and saw your post. Which supplier did you get it through. It saves a lot of stress knowing you had good results as there are heaps to choose from.<br><br>Thanks Steve<br>&nbsp;

  4. #4
    Join Date
    Sep 2021
    Location
    Adelaide
    Age
    73
    Posts
    117

    Default

    I couldn't find any in Oz, so got some from China on ebay. Not that it would have made much difference, had I found some in Oz, it would have come from China anyway.

  5. #5
    Join Date
    Oct 2019
    Location
    Adelaide, SA
    Posts
    1,220

    Default

    The photos are not clear enough to be sure its exactly what I have but I ordered something similar from SuperCheapAuto and have been using it for a while now. IIRC, It just costed 5 or 6 Aussie bucks back then and it was ready for pickup at my local store in a couple of days.

    Just search for "Car Builders Fleece Tape". I remember spending a long time searching for cloth tape but the results always showed results from overseas suppliers.

    https://www.supercheapauto.com.au/p/...=en_AU&start=2

    Capture.JPG

    Appears to be the same thing that the OP has posted.

    Here is a product demo:

    https://www.youtube.com/watch?v=eqjkFsv1M_k

  6. #6
    Join Date
    Apr 2013
    Location
    Mornington Peninsular
    Posts
    23

    Default

    If you do a search on eBay for:

    Tesa Tape 51036 High Temp 150c Engine Bay Wiring Cable Looms Wiring Harnesses

    Comes up with an Aussie supplier. Not cheap but top quality.


    Sent from my iPad using Tapatalk

  7. #7
    Join Date
    Sep 2021
    Location
    Adelaide
    Age
    73
    Posts
    117

    Default

    Quote Originally Posted by Reidy41 View Post
    I was looking for cloth tape today and saw your post. Which supplier did you get it through. It saves a lot of stress knowing you had good results as there are heaps to choose from.

    Thanks Steve
    I ordered a few rolls from different Chinese suppliers, but this stuff goes a long way. The roll I'm using at the moment is really good stuff, very, very sticky, you have to be careful not to tear it when unwinding off the roll. I had to remove some from another harness I made, not very successful and quite difficult as I couldn't see where the end was to start unravelling, so I had to cut it open then peel it off. incredibly sticky clumps of cloth and glue stuck in places so I had to use alcohol to remove it. Very impressive stuff.

  8. #8
    Join Date
    Nov 2017
    Location
    Geelong, Australia
    Age
    57
    Posts
    2,666

    Default

    I happened to have the latest Autobarn cattledog open on the table at lunchtime - and saw they have a couple of flavours of cloth loom tape.

    Standard stuff (Voltage brand) https://autobarn.com.au/ab/Autobarn-...1915/p/EL33089

    Underbody type (Carbuilders brand) https://autobarn.com.au/ab/Autobarn-...--UBT/p/142430

    Interesting the comments about the cloth tape being very sticky. Many years ago I bought plastic loom tape - and it basically had no adhesive. It was intended to be stretched slightly and be able to be removed without dealing with that horrible sticky residue of normal insulation tape. It was definitely just plastic, and not a self-amalgamating type.

    Steve

  9. #9
    Join Date
    Sep 2021
    Location
    Adelaide
    Age
    73
    Posts
    117

    Default

    Many businesses advertise items they supposedly stock, but go into the store and you'll be sadly disappointed. Bunnings is a classic example. Before I head out to buy workshop stuff I generally check online to see if they have what I want, many a time, try most of the time, After driving around from outlet to outlet I return home empty handed. Then turn to ebay. And shop keepers complain about losing business to online shopping, they are their own worst enemy.

  10. #10
    Join Date
    Jun 2005
    Location
    Helensburgh
    Posts
    618

    Default

    Quote Originally Posted by Hoggo1951 View Post
    The tape had to come from China of course, couldn't find and suppliers in Oz. So many things you just can't buy in Australia, Go down the street to buy cable, terminals, bearings and so on, visit half a dozen shops and come home empty handed. No wonder everyone is turning to online shopping, usually from overseas sellers.
    You didn't look too hard, RS components have it.
    CHRIS

Similar Threads

  1. Sharpening SS cloth/fabric roller cutters
    By BobL in forum METALWORK GENERAL
    Replies: 15
    Last Post: 20th Mar 2022, 10:47 PM
  2. Insulation testing
    By lamestllama in forum ELECTRICALS
    Replies: 2
    Last Post: 14th Jan 2018, 02:04 PM
  3. Shade Cloth on Aluminium Frame
    By Mal F in forum METALWORK GENERAL
    Replies: 7
    Last Post: 6th May 2009, 06:10 PM
  4. Liquid masking tape?
    By neksmerj in forum METALWORK GENERAL
    Replies: 11
    Last Post: 10th Dec 2007, 06:14 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •