    I binned the fuel distributor I was making, too big, and made another smaller one. The design has changed a little: There are outlet spigots either side of the fuel distributer this time which feed the carbs via fuel hoses, the two outlet spigots are joined by a 4.5mm through hole. A line from the petcock feeds into small plastic filters which feed into the two brass spigots on the front of the distributor, via fuel hose, and these feed into the 4.5mm through hole.

    The brass spigots have been undercut on the face connecting to the distributor to allow for an O ring. The brass spigots are a push fit in the distributor so shouldn't leak, the O rings are just added insurance.

    This was about as neat as I could make it and certainly neater than the jumble of hoses, adapters and T pieces I had there before.

    I didn't bother polishing the ends, that was a mistake - looks unfinished, so I'll have to remove it and polish the ends.

    Here's lots of pics (as usual), including the build process.
    Attached Images Attached Images

Similar Threads

  1. Fuel distributor.
    By Hoggo1951 in forum AUTO RESTORATION
    Replies: 2
    Last Post: 25th Jul 2022, 12:00 PM
  2. Fuel bowser
    By Iron triangle in forum METALWORK PROJECTS
    Replies: 10
    Last Post: 23rd Dec 2021, 12:57 AM
  3. Distributor advance curve
    By morrisman in forum AUTO RESTORATION
    Replies: 3
    Last Post: 12th Nov 2021, 12:06 PM
  4. Old Fuel in a MC tank
    By BobL in forum AUTO RESTORATION
    Replies: 1
    Last Post: 9th Oct 2019, 02:09 PM
  5. Fuel Tanks
    By Goggomobile in forum AUTO RESTORATION
    Replies: 9
    Last Post: 7th Jul 2016, 08:06 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •