Just my approach, I would pick up the phone instead of email and have a chat. I think the personal approach gets things moving very quickly and five minutes of phone is worth a month of back and forth emails. I also find that establishing a personal link by phone occasionely after the first call is a positive thing as well. Our engine builder was in NZ and I was always on the phone to him, sometimes daily and it paid off because we got good results.
CHRIS
-
25th May 2020, 06:56 PM #18Senior Member
- Join Date
- May 2019
- Location
- Picnic Point, Sydney
- Age
- 77
- Posts
- 312
Phoning was no doubt the best way to first communicate but I also wanted to send photo's. That's probably possible for most people but I have no idea how to send a text message on my phone.
-
25th May 2020, 07:02 PM #19Golden Member
- Join Date
- Jun 2005
- Location
- Helensburgh
- Posts
- 618
You and me both, up until recently my mobile phone lived in the car and I used to look at it every few months to check it was still on. Sadly these days I have to re-learn life with a mobile due to new business commitments and I still haven't worked out how to do more than talk on it.
CHRIS
-
25th May 2020, 11:52 PM #20
If you do happen to find a set of second hand DCOE Weber’s they will most likely need a full rebuild, the cost for this is high and finding someone good these days is hard.
New DCOE’s are expensive and there are a lot of cheaper reproductions that have a reputation for being not quite right with passages in the wrong location, making tuning difficult sometimes impossible.
There are fuel injection setups that are based on DCOE body styles https://www.efihardware.com/products...hrottle-bodies
you end up with something that looks very old school but you enjoy the tuning and drivability of EFI.
-
26th May 2020, 07:13 PM #21Senior Member
- Join Date
- May 2019
- Location
- Picnic Point, Sydney
- Age
- 77
- Posts
- 312
Where to from here? Apparently getting an engineer to certify an individually constructed vehicle (ICV) in NSW is almost impossible and if you can find that engineer he will be extremely expensive. So it appears I have a track day car unless ICV legislation changes in NSW or I try to get interstate rego. I do want to restore this car but a lot of the incentive has gone and what ever money I spend now is probably wasted.
-
26th May 2020, 07:22 PM #22Golden Member
- Join Date
- Jun 2005
- Location
- Helensburgh
- Posts
- 618
So, no VIN or chassis number I presume or any possibility of getting one? Have you been able to ascertain any history? As a way out idea the hot rod guys have some arrangement for new cars that are self built, I wonder how they do that. Have a rat through this link to see if it is applicable to your case https://www.google.com/search?client...UTF-8&oe=UTF-8
CHRIS
-
27th May 2020, 08:34 PM #23Senior Member
- Join Date
- Dec 2010
- Location
- Syd
- Posts
- 492
Originally Posted by Snapey
A friend was getting a bike engined clubman engineered with someone in the central west - which I thought was impossible from an emissions standpoint - might ask if he got any dollar figure there, or has a contact, if you want to pursue it further.
-
27th May 2020, 08:49 PM #24Golden Member
- Join Date
- Jun 2005
- Location
- Helensburgh
- Posts
- 618
I sold a car to a guy who had built a Cobra and had to hire Oran Park to do a brake test. He had the money so it didn't worry him too much, he was just p'd of that he had to go too so much trouble.
CHRIS
-
27th May 2020, 09:09 PM #25Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,942
I got asked to do a roll bar for a fibreglass VW Beach Buggy, that got defected, it was quite an effort that the vehicle had to go through. The plates to the floor was OK, but the bracing plates had to be about 150mm square,8mm thick with a 25mm radii on the corners, so that they wouldn't punch through the back into the engine bay. The plates there had to be the same size, but could be 3mm thick and HT Bolts holding it all together.
Also used to do VW Golf conversions into convertibles, and a Camaro into a convertible, the floor ended up at about 28 mm thick, as it had to be braced with 25 X 50 X 3mm RHS with 1.6 sheet on top, plus another 1.6 sheet welded underneath. It was set up on some I Beams with hydraulic jacks, chains and clamps on the vehicle to the beams, with Dial Indicators at about 20 different points, for a twisting test, it did pass, but only just.
These were engineered by Tonkin Engineering in Adelaide, I did have the actual contacts name, but it eludes me ATM, if this was any help.
KrynTo grow old is mandatory, growing up is optional.
-
27th May 2020, 09:30 PM #26Senior Member
- Join Date
- May 2019
- Location
- Picnic Point, Sydney
- Age
- 77
- Posts
- 312
That would be Treeve from Orange. It was him who posted on one of the clubman forums about the almost impossible situation regarding IVO's in NSW. I'd be interested to see how your friend got on but unfortunately I've given up on getting mine registered so it's now just a restoration project.
-
28th May 2020, 06:53 AM #27Senior Member
- Join Date
- Dec 2010
- Location
- Syd
- Posts
- 492
Sounds about the right area.
He sold, or maybe still has that clubbie on the market. Due to a long-term medical condition worsening, he had to give the project away finally about a year or 18 months ago. I don't recall how far he progressed in the bureaucratic jungle in the end, but I'll ask.
-
28th May 2020, 11:48 AM #28Golden Member
- Join Date
- Jun 2005
- Location
- Helensburgh
- Posts
- 618
A bike engine in a road car is hard to do because of no reverse gear but there have been work arounds done.
CHRIS
-
28th May 2020, 05:59 PM #29Senior Member
- Join Date
- May 2019
- Location
- Picnic Point, Sydney
- Age
- 77
- Posts
- 312
It appears that this car has never been on the road judging by the condition of the parts I've removed. Just about everything looks new but it's also been parked for a long time so both front & back brakes will need replacing or hopefully just kits for the front calipers. Today I took the last piece off the frame so tomorrow I can begin painting or at least preparing.
Progress so far,DSCN0905.jpgDSCN0906.jpgDSCN0907.jpg
-
28th May 2020, 06:25 PM #30Golden Member
- Join Date
- Jun 2005
- Location
- Helensburgh
- Posts
- 618
I wonder if it has been privately imported and they then found out it could not be registered with no numbers.
CHRIS
Similar Threads
-
My Hercus 9 Resto Start!
By wm460 in forum THE HERCUS AREAReplies: 16Last Post: 19th Aug 2022, 08:13 PM -
Mars lathe resto
By canplaythegame in forum METALWORK GENERALReplies: 7Last Post: 22nd Jan 2020, 01:35 AM -
SA-Old Imperial Mics for parts/resto-FREE
By racingtadpole in forum METALWORK - Machinery, Equipment, MARKETReplies: 2Last Post: 3rd Dec 2019, 06:13 PM -
Gmf bench grinder resto
By china eyes in forum METALWORK PROJECTSReplies: 10Last Post: 14th Apr 2019, 08:51 PM -
Resto of A model in SA
By electradaz in forum THE HERCUS AREAReplies: 7Last Post: 1st Sep 2010, 08:16 PM