30th bell
I have now made 30 successful bells. The bell pictured was 26.5 kgs with the riser and the largest I can do with my present gear. my next 2 bells will be about 50kg each so I have had to build a new furnace to take an A120 crucible, and all the gear to handle this mother of crucibles.
forumbell2.jpgforumbell.jpgforumbell1.jpgforum1.jpg
-
29th Jan 2022, 09:22 PM #2
Looks good Vin. Where do your bells end up? I can picture them on river boats but the market there is probably somewhat limited these days.
Cheers, Bob the labrat
Measure once and.... the phone rings!
-
29th Jan 2022, 10:09 PM #3Intermediate Member
- Join Date
- Mar 2006
- Location
- Waikerie SA
- Posts
- 39
At present I am building a 25 bell carillon, just because I can, I have been at it now for around 12 months, I have only 2 bells to go and then I start building the carillon frame and batten mechanism. I am not doing it for any commercial value just an expensive hobby! just ask the wife
-
30th Jan 2022, 08:47 PM #4China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,658
Vin interesting not a common thing, do yo do the machining as well, look forward to seeing some more progress when it happens.
-
31st Jan 2022, 11:50 AM #5Intermediate Member
- Join Date
- Mar 2006
- Location
- Waikerie SA
- Posts
- 39
-
1st Feb 2022, 12:21 AM #6China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,658
Yep I guess I am referring to tuning I know nothing about making bells, when I was many many moons younger I was living in Cowandilla and the next door neighbor used to make brass bells, I just remember
he used to mount them in a lathe and machine them.
-
1st Feb 2022, 10:46 AM #7
I had to look up the meaning of carillon and am surprised I hadn't come across it before.
How do you tune the bells? Is the tone mostly decided by size?Cheers, Bob the labrat
Measure once and.... the phone rings!
-
1st Feb 2022, 05:59 PM #8Intermediate Member
- Join Date
- Mar 2006
- Location
- Waikerie SA
- Posts
- 39
Diameter and thickness change a bells pitch. the larger the bell the lower the pitch, the thicker the bell the higher the pitch. So in brief you get somewhere near the pitch you want by its size make it extra thick so you can thin the inside of the bell and drop the tone. you can only tune a bell down never up
-
2nd Feb 2022, 12:31 PM #9Mechanical Butcher
- Join Date
- Oct 2004
- Location
- Southern Highlands NSW
- Posts
- 1,898
What material are Vin's bells made of?
I think the best sounding ones are of bronze.
I was delighted to find in Perth, a building that housed bells that had been taken out of the St Martin in the Fields church in London.
They were a "worn out" set but complete. Some were cracked and unringable, others were in good nick.
They even let me ring one by pulling on its pulley rope.
I was told they were gifted for the bicentennial year.
Church type bells are still being made in UK and Russia, as far as I know.
-
2nd Feb 2022, 05:00 PM #10Intermediate Member
- Join Date
- Mar 2006
- Location
- Waikerie SA
- Posts
- 39
Similar Threads
-
Casting pewter bell
By robertjenkins in forum THE FOUNDRYReplies: 4Last Post: 19th Jan 2022, 11:46 AM -
Junkyard steel - The bar bell bar material ?
By topari in forum METALWORK GENERALReplies: 18Last Post: 6th Apr 2018, 09:15 AM -
Whitleys Engineering and Fabrication Toowoomba - Onsite auction Saturday 30th July
By MasterSpoon in forum EBAY, GUMTREE, and other off forum sales sitesReplies: 1Last Post: 26th Jul 2016, 03:43 PM -
Machinery Display - May 27th to 30th
By snowyskiesau in forum METALWORK GENERALReplies: 0Last Post: 27th May 2008, 05:29 PM