Looking for a cheap beginning electric foundry a bit wider than normal
I'm just getting into casting. I mostly plan to start melting scrap aluminum, such as cans and whatever I have lying around. I don't want to invest a bunch of money at the moment so I was looking at a small cheap electric foundry. They seem to be plentiful and around $200-$300. One of those cheap Chinese ones like this:
814wrSqYTpL._AC_SL1500_.jpg
But I'm guessing because they are cheap and electric, the crucible is tall and thin. They come in various sizes, with the largest being 5kg. But it seems the crucible even for the largest one is not wide enough for an aluminum can. I'm thinking any scrap I use is going to have to be cut and that's going to be a pain for some of the larger scrap. I've seen some foundries that have space for a wider crucible and still 5kg but more expensive and gas. I could build my own but that's time I don't really have so I was hoping to find one. Any recommendations would be appreciated. I'm US based.
-
22nd Apr 2021, 09:01 AM #2Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
You will have to get used to cutting scrap up anyway. If is solid Al scrap then a wood working table saw with a negative raked toothed blade will be the quickest way to do this but it does generate a lot of swarf - which you can put into the foundry.
Not sure you should be putting whole cans inside such a small foundry anyway because off the have any liquid inside then KABOOM. That's also why crushing them down is not a good idea. I would at least cut them is half and make sure they were bone dry.
-
22nd Apr 2021, 09:15 AM #3New Member
- Join Date
- Apr 2021
- Location
- USA
- Posts
- 2
If it were just soda cans (good tip on the liquid) it wouldn't be as big an issue but I do have other scrap like old disassembled hard drives. I figured I'd probably have to do some cutting anyway but was hoping I could maybe lessen it. I have a habit of getting carried away with my hobbies so first it's getting a foundry, then something to cut, then making a dedicated space, then who knows what else, lol.
-
22nd Apr 2021, 11:45 PM #4
Not sure exactly what material HD chassis are cast from, but it's fairly likely that there is a fair range of other materials in the metal. May not be an issue for your needs, but it should be something to be considered.
I did a few small pours 40+ years ago recycling old scrap from castings etc with very crude gear and found typically about 40% by volume of the melt was semi liquid impurities floating on top of the melt. That's a lot of volume to loose. No doubt there are ways to do it with much better equipment than I was using, and producing better results, but if you don't know what goes into the pot, you probably don't know what will come out.
Ali cans tend to have printed ink on the outside, sometimes protected by a lacquer, and some form of coating inside as well.I used to be an engineer, I'm not an engineer any more, but on the really good days I can remember when I was.
-
23rd Apr 2021, 09:05 AM #5
Possibly the best bet for decent scrap Al would be automotive engine pistons.
These could be hacksawed or smashed with a hammer into small pieces.
A lot of modern Al components out there are pot metal for diecasting and similarly a lot of extrusion isn’t that flash either.
H.Jimcracks for the rich and/or wealthy. (aka GKB '88)
-
23rd Apr 2021, 11:14 AM #6Diamond Member
- Join Date
- Aug 2019
- Location
- Revesby - Sydney Australia
- Age
- 57
- Posts
- 1,196
Similar Threads
-
WTB Sheet metal roller 1m or wider- VIC
By Arty Marty in forum WANTED TO BUYReplies: 0Last Post: 19th Aug 2020, 04:56 PM -
Beginning Metalworking: Working with Aluminum on a Small Scale
By qin in forum METALWORK GENERALReplies: 15Last Post: 26th Feb 2017, 02:37 AM -
kiss a VFD a good bye . now you can run 3 phase motor on your normal 240v main
By thorens in forum METALWORK GENERALReplies: 19Last Post: 30th Nov 2013, 05:39 PM -
Is this normal.
By jonson in forum FORUMS INFO, HELP, DISCUSSION & FEEDBACKReplies: 10Last Post: 6th Aug 2011, 06:29 AM -
A project beginning
By MWMACH in forum THE HERCUS AREAReplies: 5Last Post: 22nd Mar 2010, 06:29 AM