Needs Pictures: 0
Picture(s) thanks: 0
Results 1 to 4 of 4
Thread: Smelting Brass & Ali at home
-
14th Mar 2021, 04:36 PM #121 with 19 years experience
- Join Date
- May 2004
- Location
- Sunshine Coast Queensland
- Age
- 53
- Posts
- 52
Smelting Brass & Ali at home
Smelting (or rather the ability to do it at home) has been a long held dream of mine - a cousin of dads worked at a foundry in Perth and always brought over cool stuff, and it was done at my high school although I never got to do it.
In regard to brass, my brother is a plumber so I have an ongoing source of scrap brass.
What sort of set up & cost could be involved, I've seen a camping type gas burner with an air hose attached, would that give me the temp I need?
Any information or links to aussie websites would be much appreciated.
Cheers
Smidsy
-
15th Mar 2021, 06:00 PM #2Senior Member
- Join Date
- Oct 2015
- Location
- melbourne
- Posts
- 473
Search for home foundry - smelting is turning metal ore into metal. You want to cast.
You'll need a lot more heat than a bbq style burner. But they can be fabricated.
You need a furnace, burner, crucible, lifting and pouring tongs, safety gear. Then some sort of mould, pattern, moulding sand.
All on my to-do list...
-
15th Mar 2021, 06:55 PM #3Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,183
Yep! Last year I monitored with interest my nephew have several goes at casting brass using BBQ briquettes in his small blacksmiths forge. He used spent brass bullet casings as a brass source and a 150mm long piece of 1" black pipe as a crucible and after a lot of effort and several bags of briquettes he made a few twisted blobs.
It's surprising how much heat is required - smaller heat sources can be used but then very high levels of insulation (fire brick lined chambers) are needed and it takes a long time to get it to melt.
The idea of using old bits of brass plumbing has some drawbacks. They shouldn't be used without cutting them up as any trapped water and air inside the fittings can cause explosions.
-
16th Apr 2021, 12:32 PM #4Most Valued Member
- Join Date
- Jul 2006
- Location
- Athelstone, SA 5076
- Posts
- 4,255
what..no thanks for the good advice
BobL and Russ...please accept my thanks to you both for smidsy
Similar Threads
-
what rods for thin brass to brass ??
By Mathuranatha in forum WELDINGReplies: 7Last Post: 23rd Nov 2020, 08:17 PM -
H59 brass
By morrisman in forum METALWORK GENERALReplies: 4Last Post: 19th Feb 2020, 11:33 PM -
VICTORIA Brass Flat Bar Assorted Sizes & 1/4" SWB Threaded Rod & 260 Carbide Brass Sheet
By thumbsucker in forum METALWORK - Machinery, Equipment, MARKETReplies: 7Last Post: 18th Mar 2013, 03:36 PM -
MIG brass ?? Yes or No
By Gaza in forum WELDINGReplies: 6Last Post: 13th Sep 2012, 12:48 AM -
brass
By tanii51 in forum METALWORK GENERALReplies: 3Last Post: 22nd Aug 2009, 09:21 PM