    Default centrifugal casting machine (jewelery): how build ?

    how can i build a centrifugal casting machine for gold/silver jewelry,eg, rings,etc ? thanks

  2. #2
    Join Date
    Jan 2004
    Location
    Mackay North Qld
    Posts
    6,446

    Default

    Hi qmuddy2,

    Welcome to the MetalWork Forums,
    Hopefully someone will be along to help you soon.

    We have some fine folks here who are supportive friendly and helpful.

    Please take the time to navigate around the forums to view the varied and interesting subjects.
    There is a dedicated Hercus Forum here so there is a good place to start.

    To do this, goto the the FORUM box in the top left hand corner of the screen. Click Forum Home and a scroll down page will come up.

    Scroll down the page and the various help pages and sub forums shall be shown.

    Please read the Terms of Use on the very top of the scroll down page - they are our rules.
    To save time heres the link

    https://metalworkforums.com/f90/t197...terms-tou-read

    Many pages also have a sticky at the top.If you post its always a good idea to check the sticky ,if there is one there.

    Please post your questions in the appropriate MetalWork forum.

    Again, welcome to our forums.

    Grahame

  3. #3
    Join Date
    Aug 2019
    Location
    Revesby - Sydney Australia
    Age
    57
    Posts
    1,195

    Default

    Factory neighbour uses a lathe, and a tube/mould with stepped end caps. Chuck end is sealed, tailstock end has a large enough hole to pour metal down a ramp into the tube.

    This is for pouring bearings, though. Packing with moulding sand, and ensuring the metal travels into the mould correctly, might be a little trickier

  4. #4
    Join Date
    Apr 2018
    Location
    Perth
    Posts
    168

    Default

    many years ago when I was a apprentice we used to melt down the silver contacts from large DC contactors to make jewelry. We used cuttlefish shell to make the moulds but only poured metal into them.
    might be a simple medium to make the moulds out of.

Similar Threads

  1. centifugal casting machine : how build ?
    By qmuddy2 in forum JEWELLERY
    Replies: 1
    Last Post: 24th Feb 2021, 11:25 AM
  2. Rotational casting machine
    By jhovel in forum METALWORK PROJECTS
    Replies: 8
    Last Post: 7th Apr 2016, 12:12 PM
  3. Casting about for cast iron casting ideas
    By Graziano in forum THE FOUNDRY
    Replies: 49
    Last Post: 1st Apr 2012, 12:05 PM
  4. U-Build Machine & Power Tools Catalog
    By Poorman in forum METALWORK GENERAL
    Replies: 0
    Last Post: 11th Jul 2005, 11:52 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •