    Default Babington burner for forge and foundry

    Hy guys, it is my first post on forum and I need your help with some advice for to improve my wasted oil burner temperature, My babington burner can melt cooper wire in few seconds and a cooper pot for casting in 5 minutes but the temperature obtained inside the forge is not sufficient for damascus steel making. How to improve my burner to increase the temperature at 2372 F (1300*Celsius) to obtain almost white color steel for forge welding.
    My burner use wasted oil from kitchen, car and hydraulic oil, burn 2,5 liters /hour , air pressure from compressor is 2,5 atm and I attach a short movie and a picture with it
    Attached Images Attached Images
    Attached Files Attached Files

  2. #2
    Join Date
    May 2013
    Location
    Rockhampton, QLD
    Age
    68
    Posts
    455

    Default

    Welcome to the forum.

  3. #3
    Join Date
    Jan 2004
    Location
    Mackay North Qld
    Posts
    6,446

    Default

    Hi otonel,
    Welcome to the MetalWork Forums. We are mainly of Aussie members with a sprinkling of overseas member.
    People here will help you if thy can.
    To see what on offer in the rest of the forum/s do this:

    To help you explore the other areas of our forum here's a guide on to to navigate our Forum and find all the interesting places.

    Goto the FORUM box in the top left hand cnr of the page and click the down arrow. This will bring up a pull down menu that has Forum Home at the top

    Click Forum Home which will present a scroll down page.

    Our rules,the Terms of Service are right at the top ,please read them.

    Below that are all the various areas and sub forums that make up our MetalWork forums.


    Welcome

    Grahame

  4. #4
    Join Date
    Jan 2004
    Location
    Mackay North Qld
    Posts
    6,446

    Default

    Otonel,

    It sounds like you may require a LPG burner fitted to your furnace to achieve the extra temperature.
    I don't forge so I can't talk on the basis of experience.

    A knife orientated site suggests that temperature need to be somewhere around 2000 - 2300 F - https://blademag.com/knifemaking/how-to-forge-damascus

    A blacksmith site recommends slightly different temperature of 1500- 2000F. https://blacksmithcode.com/how-to-forge-damascus-steel/

    We have a knife sub forum here so it is worth checking out.find it by going to FORUM top LH side click FORUM HOME and scroll down till you see Knife forums.

  5. #5
    Join Date
    Dec 2009
    Location
    Sydney
    Posts
    327

    Default

    Greetings otonel!
    Here is a couple of helpful Australian videos;
    demonstration of home-made burner, https://youtu.be/1SXKMRSIyPU
    and
    how it is put together, https://youtu.be/iW1odjaM8w8

    hope this helps you.
    Regards,
    Andrew

Similar Threads

  1. Gas burner
    By Maxi77 in forum THE FOUNDRY
    Replies: 7
    Last Post: 15th Apr 2017, 03:45 AM
  2. Oil burner
    By phaser in forum THE FOUNDRY
    Replies: 6
    Last Post: 16th Nov 2016, 10:47 AM
  3. Replies: 1
    Last Post: 10th Nov 2015, 12:07 PM
  4. burner help
    By fxst in forum THE FOUNDRY
    Replies: 4
    Last Post: 21st Jun 2013, 12:36 AM
  5. Forced Air LPG Burner Mk2
    By RayG in forum THE FOUNDRY
    Replies: 26
    Last Post: 6th Jun 2011, 12:50 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •