Which bolt into cast iron in firebox?!
Bit of a weird one this, but hoping someone here will know the answer!
I have a problem with my wood stove. The cast iron baffle plate basically just rests on a couple of tabs at the front and the wetback tank at the back. The problem is if it gets knocked when loading a log, it pops up and slides back over the wetback and drops off its front tabs into the firebox. As you can imagine, much hilarity ensues.
After much thought, the only practical solution I can come up with is to tap a thread into the plate at the back, and insert a bolt. The bolt can just snug up to the structure above and stop the baffle plate from being pushed up.
I know that tapping the cast iron plate is doable. What I'm not sure about is how to ensure a long service life from the bolt in the hostile environment of a hardworking redgum-fuelled firebox. Obviously it needs to be removable for future cleaning and servicing.
I was thinking of using a stainless bolt as in my experience stainless tends to hold up better to intense heat than mild steel. But I don't know whether differential expansion or galvanic action or some other vector will cause trouble over time. Is there a particular type of bolt that is a best choice for this application?
-
5th Sep 2020, 01:14 PM #2Most Valued Member
- Join Date
- Jul 2016
- Location
- Melbourne
- Age
- 35
- Posts
- 1,522
Considering tthere is no load you could make a cast iron bolt.
-
5th Sep 2020, 08:52 PM #3Most Valued Member
- Join Date
- Jun 2007
- Location
- sydney ( st marys )
- Age
- 64
- Posts
- 4,890
Based on what you are looking to do I am not sure if cast iron would be a good choice for your locating bolt,Stainless might be the better alternative.
If the locating bolt/ support needs to be removed periodically even a through hole through your damper with a bolt with nut top and bottom may work.
-
5th Sep 2020, 11:34 PM #4Novice
- Join Date
- Apr 2008
- Location
- Southern Riverina
- Posts
- 24
Thanks guys, I may be totally overthinking this, I just don't want to have to try and drill out a buggered bolt at the back of the firebox the next time I need to replace some bricks. I think I'll go with a stainless bolt and maybe a smear of copper antiseize just for fun.
-
6th Sep 2020, 09:38 AM #5
Similar Threads
-
WTB-Cast Small Cast Iron Lapping Plate
By Betnorm in forum WANTED TO BUYReplies: 4Last Post: 19th Nov 2019, 01:01 PM -
When does cast iron not machine like cas t iron?
By simonl in forum METALWORK GENERALReplies: 20Last Post: 31st Jul 2018, 08:57 PM -
Cast iron fireplace - Question for restoring using Penetrol & Liberon Iron Paste
By mookschank in forum METALWORK GENERALReplies: 8Last Post: 19th Jun 2013, 06:32 PM -
Cast iron VS Cast steel lathe compound slide
By Ueee in forum METALWORK GENERALReplies: 10Last Post: 23rd Dec 2012, 11:40 PM -
Cast Iron
By RayG in forum METALWORK GENERALReplies: 17Last Post: 30th Apr 2011, 02:27 PM