Aluminium Castings - Flux and melt Gas release alternatives
Hi guys,
i was watching myfordboy on youtube casting aluminium.
i note that he uses salt and washing soda for flux and removing gases from the molten aluminium.
Has anyone tried this, does it work as successfully as it seems to for myfordboy.
-
30th Jul 2020, 11:07 PM #2China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,658
Most casters I know use borax
-
30th Jul 2020, 11:47 PM #3
Bluey purple coloured tablets, probably borax.
Ive possibly got the TAFE notes in the stash somewhere.
H.Jimcracks for the rich and/or wealthy. (aka GKB '88)
-
1st Aug 2020, 11:27 AM #4Golden Member
- Join Date
- Apr 2018
- Location
- Drouin Vic
- Posts
- 634
I have used them and they seem to work just fine- although I am far from an authority. Lite salt is the stuff to use for flux- it is a blend of sodium chloride and potassium chloride. I wrap about a tablespoon of it in some alfoil, drop it into the pot and stir it in. Sodium carbonate- laundry soda- wrapped the same way and plunged into the bottom of the pot certainly brings a lot of bubbles to the surface. I bought some commercial stuff a few years ago but I have to travel half a day to any foundry supply so use DIY solutions.
Similar Threads
-
Is lathe bed grinding available in Brisbane? Any alternatives?
By j3dprints in forum METALWORK GENERALReplies: 11Last Post: 12th May 2018, 06:18 PM -
Alternatives to stainless acid pickles
By Michael G in forum WELDINGReplies: 24Last Post: 18th Jun 2017, 10:44 AM -
Welding Alternatives.
By soundman in forum WELDINGReplies: 0Last Post: 8th Oct 2014, 10:35 AM -
how can you melt aluminum without a furnace
By welder in forum THE FOUNDRYReplies: 10Last Post: 2nd Oct 2012, 07:34 PM -
Anodising or alternatives in the shed
By Michael G in forum METALWORK GENERALReplies: 7Last Post: 3rd Jun 2012, 03:13 PM