    I am planning on casting an engagement ring that will house one round cut diamond. It will have the pieces sticking out for the stone's setting. If cost is a factor, what is the best method for casting this ring? It is for a friend of mine so I don't want to mess up.

  2. #2
    Join Date
    May 2011
    Location
    Murray Bridge S Aust.
    Age
    69
    Posts
    4,904

    Default

    Welcome to a TOP FORUM from Down Under.
    Sorry, I can't help with your question, but we have a seperate section for Jewelry making, you might be better off asking there.
    Have added a link to assist you. https://metalworkforums.com/f310
    Kryn
    To grow old is mandatory, growing up is optional.

  3. #3
    Join Date
    Feb 2009
    Location
    Adelaide - outer south
    Age
    65
    Posts
    9

    Default

    Clay casting is similar to casting in sand moulds in the sense that there is a parting line. This would probably not allow you to mould all the features that you need, such as the claws that hold the stone. Investment casting may cost more but also may be the only way to cast what you need.
    Cheers, Bob the labrat

    Measure once and.... the phone rings!

Similar Threads

  1. Melting brass for lost wax casting
    By inlay chris in forum THE FOUNDRY
    Replies: 4
    Last Post: 17th Jun 2016, 09:06 PM
  2. Casting about for cast iron casting ideas
    By Graziano in forum THE FOUNDRY
    Replies: 49
    Last Post: 1st Apr 2012, 12:05 PM
  3. Casting Tools Part 4 - Sand Casting Tools
    By RayG in forum THE FOUNDRY
    Replies: 8
    Last Post: 9th Dec 2011, 12:03 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •