10th Jan 2020, 01:17 AM #1China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,657
Sand casting
I have done lots of sand casting, ( only small items ) I have a question, if one was making just a rectangular strip, I assume there would be no reason to center the pattern in the mould i.e. just place it one half and have the other half just a flat surface.
-
10th Jan 2020, 06:55 AM #2Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,559
Correct. A foundry would probably prefer it that way, as it is less work to make up the mould.
Michael
-
10th Jan 2020, 08:47 AM #3Senior Member
- Join Date
- Aug 2011
- Location
- Perth, Western Australia
- Age
- 67
- Posts
- 362
-
10th Jan 2020, 01:04 PM #4China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,657
Thanks for the replies, several people told me it can't be done that way, I did not see any reason why not
-
10th Jan 2020, 01:47 PM #5Senior Member
- Join Date
- Aug 2011
- Location
- Perth, Western Australia
- Age
- 67
- Posts
- 362
Unless its more complicated than my understanding of it why would you want to have a parting line on a strip. Means you would have to double tapper the pattern as well.
Tony
-
10th Jan 2020, 10:30 PM #6Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,959
My understanding of what you're wanting to do is cast something like an ingot, an indent in the sand and molten metal poured in and hey presto. Some lead fishing sinkers are cast in a similar way.
HTH
KrynTo grow old is mandatory, growing up is optional.
-
10th Jan 2020, 11:28 PM #7China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,657
Similar to a ingot except I want to get it more precise ( less finishing ) I know you can do it by the open casting method and I am aware that it can be done by the usual half and half method, I just don't see any point in the half and half method when it is just a long rectangular piece.
I mentioned it at a gathering of friends and the advice came flowing even though apparently non of them has ever cast anything, so I thought I would consult the oracle before I made some horrible mistake as I mentioned I have cast lots of things, about the only thing I have not cast is rectangular strip.
-
10th Jan 2020, 11:53 PM #8Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,959
I'd give it a try and see what happens, you've nothing to loose but a bit of your mold material and Electrickery, as what you cast, will be able to be remelted and cast again.
Let us know how you get on PLEASE.
KrynTo grow old is mandatory, growing up is optional.
-
11th Jan 2020, 12:04 AM #9Senior Member
- Join Date
- Aug 2011
- Location
- Perth, Western Australia
- Age
- 67
- Posts
- 362
The 1 piece open top mould will never produce as good a finish on the open section as closed 2 piece mould.
Tony
-
11th Jan 2020, 12:37 AM #10China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,657
Yep no probs will post a pic or two
Similar Threads
-
Regenerating oil bound casting sand
By MuellerNick in forum THE FOUNDRYReplies: 11Last Post: 20th Jan 2013, 09:24 PM -
Vacuum assisted casting in core-sand moulds.
By MuellerNick in forum THE FOUNDRYReplies: 22Last Post: 30th Oct 2012, 03:09 PM -
Casting about for cast iron casting ideas
By Graziano in forum THE FOUNDRYReplies: 49Last Post: 1st Apr 2012, 12:05 PM -
Casting Tools Part 4 - Sand Casting Tools
By RayG in forum THE FOUNDRYReplies: 8Last Post: 9th Dec 2011, 12:03 PM -
is the sand from a sand blaster carcinogenic???
By new_guy90 in forum METALWORK GENERALReplies: 12Last Post: 24th Nov 2010, 10:09 PM