    Over on the WW Forum, Hand Tools -Unpowered - unusual brace, we were talking about a brace patentee Nelson Spoffard and a statement he made in an 1880 patent.

    A patent update in March 1880 (US Pat 22768) Spofford rejects sawing the division in favour of casting it forked because "to preserve the strength and resiliency of an article made of cast metal it is necessary to preserve the skin of the casting intact, as the thin hard covering or skin that envelops the casting has the effect of imparting increased strength to the same. Hence, when the slit is formed in the arm of the bit-brace by cutting the metal away with a milling device, the interior portions of the arms are left without the skin metal that surrounds the outer portions of the arm, and thus the slitted arms materially weakened and their resiliency lessened to a considerable degree".

    How accurate would you foundry aficionados think this statement is?
    Cheers,
    Geoff.

  2. #2
    Join Date
    Jul 2016
    Location
    Melbourne
    Age
    31
    Posts
    1,052

    Default

    Basically any introduction of a sharp internal feature will always be a concentration for stresses. I think its more the inherant radius in the casting than the actual skin which is providing the strength.

  3. #3
    Join Date
    Dec 2007
    Location
    Sydney
    Posts
    92

    Default

    I agree as far as rads go in any casting.
    Cast iron certainly has a hard skin and Spofford braces were CI.
    So maybe a bit of both?
    H.
    Jimcracks for the rich and/or wealthy. (aka GKB '88)

Similar Threads

  1. Technical Specification of AL340
    By oz94 in forum METALWORK GENERAL
    Replies: 25
    Last Post: 4th Dec 2014, 08:44 AM
  2. Out-of-Copyright Technical e-books
    By Blu_Rock in forum METALWORK GENERAL
    Replies: 0
    Last Post: 25th May 2014, 11:44 PM
  3. technical drawing
    By tanii51 in forum METALWORK GENERAL
    Replies: 6
    Last Post: 1st Dec 2009, 06:56 PM
  4. Replies: 10
    Last Post: 21st Apr 2008, 09:53 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •