    Default Recipe for ceramic cement

    Does anyone have a recipe for a ceramic cement for lining a small kiln for melting aluminium and or brass?

    Thanks in advance

  2. #2
    Join Date
    Apr 2007
    Location
    Adelaide Hills
    Posts
    9

    Default

    Quote Originally Posted by alfclp View Post
    Does anyone have a recipe for a ceramic cement for lining a small kiln for melting aluminium and or brass?

    Thanks in advance
    Start with https://www.pugmill.com.au/adelaide-ceramic-specialist

    eg. https://www.pugmill.com.au/shop/air%...tail/offset/0?

    There may be cheaper sources, so also search for other pottery suppliers.
    Neil

    Time for a new signature line... just waiting on inspiration

  3. #3
    Join Date
    Sep 2007
    Location
    Wentworth Falls NSW 2782
    Age
    77
    Posts
    134

    Default

    It should be possible to buy a bag of fireclay but if you want to just mix your own, a 1:1 mix of Plaster of Paris and sand can be used.
    Not sure how long it would last though.
    This is a You Tube of a guy making a small forge but could just as easily be used as a furnace

    https://www.youtube.com/watch?v=Po9EKcOj1uc

    Many of his videos are worth watching.

    Hope this helps,

    Findlay

Similar Threads

  1. Drill Press Table Refurbishment ( Or A Recipe For Disaster? )
    By Anorak Bob in forum METALWORK GENERAL
    Replies: 33
    Last Post: 30th Jul 2019, 04:50 PM
  2. Recipe for homemade Way Oil
    By KBs PensNmore in forum METALWORK GENERAL
    Replies: 6
    Last Post: 6th Jun 2019, 10:43 AM
  3. Ceramic fiber rigidizer, where to buy?
    By Com_VC in forum THE FOUNDRY
    Replies: 6
    Last Post: 7th Sep 2016, 10:57 PM
  4. re ceramic blanket
    By texx in forum THE FOUNDRY
    Replies: 11
    Last Post: 5th Sep 2013, 10:47 PM
  5. Calcium Aluminate Cement
    By Stustoys in forum THE FOUNDRY
    Replies: 3
    Last Post: 18th Jul 2013, 08:03 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •