    Default Colloidal silica for ceramic shell casting - who supplies it?

    Has anyone found a source, in Australia, of colloidal silica, as used for ceramic shell investment casting?

    If no luck here I'll see if I can wheedle that info out of one of the art bronze foundries - it seems that this is their favourite casting technique.

    BTW if anyone is curious, I found an older book (1980) that has a good detailed how-to process description for this technique in a back shed or college situation - "Methods for Modern Sculptors" by R.D. Young and R.A. Fennell. See Trove.nla.gov.au for library holdings.

  2. #2
    Join Date
    Dec 2007
    Location
    Sydney
    Posts
    399

    Default

    Barnes pattern supplies up here in Sydney used to supply stuff for Shaw process casting system.
    On Kevin’s passing his daughter has gone more into stuff for the film etc industry but they might be worth a call.
    A bloke I know up Bathurst was using this for sculptural stuff, I’m not at all conversant with the process personally.
    H.
    Jimcracks for the rich and/or wealthy. (aka GKB '88)

  3. #3
    Join Date
    Jul 2006
    Location
    Canberra
    Posts
    288

    Default

    I found Barnes on the net, Moulding, casting & sculpting supplier in Aus & NZ - Barnes Products. They have all their products online. Very good, exhaustive even, for silicon mould-making supplies. Unfortunately nothing there that is used for ceramic shell casting.

    I've sent emails to a couple of the Sydney art-bronze casting outfits, asking for their source. We'll see if either one replies.

  4. #4
    Join Date
    Jul 2006
    Location
    Canberra
    Posts
    288

    Default

    So one of the art foundries did reply, saying that they buy it from Foseco in Padstow.

    I called Foseco in Padstow, (the call was transferred to Foseco in Dandenong Vic so it's the same story for either branch) and they do sell it, but only by the 150kg drum (it's a slurry). Price is $11.05/kg, ex-gst, so drum is $1823 inc gst. The other thing is that they state the shelf life is 12 months.

    Unless any new info comes to light, the non-availability of smaller amounts, and the limited shelf-life preventing stockpiling or ebaying the excess, seems to kill the possibility of backyard ceramic shell casting in Australia. As the well-known US idiot Donald Trump would say, SAD!

  5. #5
    Join Date
    Dec 2007
    Location
    Sydney
    Posts
    399

    Default

    Google ‘Shaw process’.
    They are in Mortdale.
    They have a web site which may or not be helpful.
    H.
    Jimcracks for the rich and/or wealthy. (aka GKB '88)

  6. #6
    Join Date
    Jul 2006
    Location
    Canberra
    Posts
    288

    Default

    Thanks, I had a look at their website - that's pretty much the nirvana of industrial ceramic shell casting (or are they doing ceramic mold casting, i.e. literally using the shaw process, so not just their business name. I can't tell).

    I suppose with these commercial investment casting foundries, whether industrial or art, it might be possible to buy a few kg of their bulk supply of colloidal silica. I've emailed that question to one of them. Maybe they'll answer, or not.

  7. #7
    Join Date
    Apr 2011
    Location
    rockhampton qld australia
    Posts
    7

    Default casting supplies

    i buy colodial slica and zircon flour from Castmetal services. And also the stucco .
    The colodial i buy comes in a 20 litre Bucket

Similar Threads

  1. Cutting Oil - Shell Dromus Oil BL - 20L
    By John T K in forum METALWORK - Machinery, Equipment, MARKET
    Replies: 1
    Last Post: 15th Oct 2017, 11:38 PM
  2. Hydraulic oil ISO 32 - like Shell Tellus
    By GeoffW1 in forum METALWORK GENERAL
    Replies: 4
    Last Post: 11th Sep 2016, 09:35 AM
  3. SHELL TONNA OIL 27 in QLD
    By iron bark in forum METALWORK GENERAL
    Replies: 4
    Last Post: 27th Jan 2014, 06:37 AM
  4. re ceramic blanket
    By texx in forum THE FOUNDRY
    Replies: 11
    Last Post: 5th Sep 2013, 10:47 PM
  5. Casting about for cast iron casting ideas
    By Graziano in forum THE FOUNDRY
    Replies: 49
    Last Post: 1st Apr 2012, 12:05 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •