Likes Likes:  0
Needs Pictures Needs Pictures:  0
Picture(s) thanks Picture(s) thanks:  0
Results 1 to 6 of 6
  1. #1
    Join Date
    Nov 2013
    Location
    Far North, NZ
    Posts
    10

    Default Reil burner piping

    Hi all, am just looking at making a propane powered smelter. I have found the Reil burner and it seems to be what I'm after.
    Does the piping have to be black steel nipples or can galv be used without health or quality risks?

  2. #2
    Join Date
    May 2011
    Location
    Murray Bridge S Aust.
    Age
    71
    Posts
    5,959

    Default

    I would say that the fittings should be black steel. Using galv would be a health and quality risk.
    Kryn
    To grow old is mandatory, growing up is optional.

  3. #3
    Join Date
    Nov 2013
    Location
    Far North, NZ
    Posts
    10

    Default

    Thanks Kyrn, will have to look a bit further around, cheers.

  4. #4
    Join Date
    Feb 2013
    Location
    Laidley, SE Qld
    Posts
    1,039

    Default

    I have an LPG burner that I made from 1/2" gal water pipe, the only gal that has disappeared is from the part of the burner within the furnace.

  5. #5
    Join Date
    Aug 2015
    Location
    Plainland Qld Australia
    Posts
    5

    Default

    Quote Originally Posted by bob ward View Post
    I have an LPG burner that I made from 1/2" gal water pipe, the only gal that has disappeared is from the part of the burner within the furnace.
    I have read that the zinc gavanising is really bad for you, gives off undesireable fumes but if you soak the gal fittings in Hydrochloric acid it wont be galvanised for very long
    Vaughng

  6. #6
    Join Date
    Oct 2015
    Location
    melbourne
    Posts
    473

    Default

    You only need to strip the zinc for a couple of inches.
    Or light it up and leave for 20 minutes...

Similar Threads

  1. Gas burner
    By Maxi77 in forum THE FOUNDRY
    Replies: 7
    Last Post: 15th Apr 2017, 03:45 AM
  2. Oil burner
    By phaser in forum THE FOUNDRY
    Replies: 6
    Last Post: 16th Nov 2016, 10:47 AM
  3. burner help
    By fxst in forum THE FOUNDRY
    Replies: 4
    Last Post: 21st Jun 2013, 12:36 AM
  4. Forced Air LPG Burner Mk2
    By RayG in forum THE FOUNDRY
    Replies: 26
    Last Post: 6th Jun 2011, 12:50 AM
  5. Sealing gas inlets on wok burner
    By R. McCarthy in forum METALWORK GENERAL
    Replies: 16
    Last Post: 18th Jan 2008, 09:08 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •