Melting brass for lost wax casting
I've been trying to cast intricate ormolu mounts for the miniature furniture I make..
I've worked out the modelling, wax injecting OK and am very happy with this part but the metal is my big problem...
Firstly I bought myself a spin casting machine and burnout kiln, OK so far..
I then tried and failed to melt brass, the castings have to be gold anyway and it seemed the obvious choice. Sadly I've been unable to melt it effectively. I've used propane, butane and mapp gas which worked to a degree but was still unreliable. I thought the trouble was the small crucible dissipating the heat.
With this in mind I started using aluminium to start with and then pewter because of the low melting point...I now have serious electro plating problems which has been driving me mad...
Yesterday I bought a rothenberger oxy propane setup thinking this should surely crack the problem but still won't melt the brass. How much more time and money do I have to spend solving this 10 year problem? Any ideas would be very welcome.
It can be any gold coloured metal....
-
5th May 2016, 08:12 AM #2Member
- Join Date
- May 2009
- Location
- Somerset, UK
- Posts
- 60
I've cast brass OK using propane (BIG Burner) in a home made crucible furnace (Think 12in steel cylinder lined with fire cement and a hole in the side for the burner)
One thing to be aware of with brass are the zinc fumes that are generated - nasty stuff
Oh yes - make sure the moulds are well burnt out - not doing so gave me some interesting results...............
MarkLast edited by Old-Biker-UK; 5th May 2016 at 08:14 AM. Reason: CRAFT moment
What you say & what people hear are not always the same thing.
http://www.remark.me.uk/
-
5th May 2016, 04:26 PM #3New Member
- Join Date
- May 2006
- Location
- uk
- Age
- 59
- Posts
- 2
The only problem I have is I'm spin casting so the melt has to be in the crucible mounted on the machine. I'm going to give a mapp gas oxy mix a try and get that extra heat...
Worked on the burnout and don't take shortcuts, I've had a few messups before because of 'finning' etc and my workshop still have molten metal stuck to the walls to prove it...
I like the idea though..Maybe I can rig up a fire brick cage I can remove just before spinning the machine?
-
7th May 2016, 09:53 PM #4Diamond Member
- Join Date
- Feb 2013
- Location
- Laidley, SE Qld
- Posts
- 1,038
If you've not been there, alloyavenue.com is a great source of info for all things DIY metal casting, the melting of brass is a well covered subject.
-
17th Jun 2016, 09:06 PM #5
Why can't you melt the metal in another furnace/crucible and then pour it into the crucible on the machine?
Can you post a pic of the machine? It may help to illustrate the limitations / possibilities.Cheers, Bob the labrat
Measure once and.... the phone rings!
Similar Threads
-
Anyone have any experience casting brass?
By Jim Ferrous in forum METALWORK GENERALReplies: 7Last Post: 27th Sep 2013, 02:32 PM -
VICTORIA Brass Flat Bar Assorted Sizes & 1/4" SWB Threaded Rod & 260 Carbide Brass Sheet
By thumbsucker in forum METALWORK - Machinery, Equipment, MARKETReplies: 7Last Post: 18th Mar 2013, 03:36 PM -
Casting about for cast iron casting ideas
By Graziano in forum THE FOUNDRYReplies: 49Last Post: 1st Apr 2012, 12:05 PM -
Casting a brass nut.
By Skew ChiDAMN!! in forum METALWORK GENERALReplies: 6Last Post: 21st Nov 2011, 01:04 PM -
Wanting to get into metal melting/casting, where to start?
By Com_VC in forum THE FOUNDRYReplies: 12Last Post: 6th Nov 2011, 10:13 PM