    I've been trying to cast intricate ormolu mounts for the miniature furniture I make..
    I've worked out the modelling, wax injecting OK and am very happy with this part but the metal is my big problem...
    Firstly I bought myself a spin casting machine and burnout kiln, OK so far..
    I then tried and failed to melt brass, the castings have to be gold anyway and it seemed the obvious choice. Sadly I've been unable to melt it effectively. I've used propane, butane and mapp gas which worked to a degree but was still unreliable. I thought the trouble was the small crucible dissipating the heat.
    With this in mind I started using aluminium to start with and then pewter because of the low melting point...I now have serious electro plating problems which has been driving me mad...

    Yesterday I bought a rothenberger oxy propane setup thinking this should surely crack the problem but still won't melt the brass. How much more time and money do I have to spend solving this 10 year problem? Any ideas would be very welcome.

    It can be any gold coloured metal....

  2. #2
    Join Date
    May 2009
    Location
    Somerset, UK
    Posts
    60

    Default

    I've cast brass OK using propane (BIG Burner) in a home made crucible furnace (Think 12in steel cylinder lined with fire cement and a hole in the side for the burner)
    One thing to be aware of with brass are the zinc fumes that are generated - nasty stuff
    Oh yes - make sure the moulds are well burnt out - not doing so gave me some interesting results...............
    Mark
    Last edited by Old-Biker-UK; 5th May 2016 at 08:14 AM. Reason: CRAFT moment
    What you say & what people hear are not always the same thing.
    http://www.remark.me.uk/

  3. #3
    Join Date
    May 2006
    Location
    uk
    Age
    59
    Posts
    2

    Default

    Quote Originally Posted by Old-Biker-UK View Post
    I've cast brass OK using propane (BIG Burner) in a home made crucible furnace (Think 12in steel cylinder lined with fire cement and a hole in the side for the burner)
    One thing to be aware of with brass are the zinc fumes that are generated - nasty stuff
    Oh yes - make sure the moulds are well burnt out - not doing so gave me some interesting results...............
    Mark

    The only problem I have is I'm spin casting so the melt has to be in the crucible mounted on the machine. I'm going to give a mapp gas oxy mix a try and get that extra heat...
    Worked on the burnout and don't take shortcuts, I've had a few messups before because of 'finning' etc and my workshop still have molten metal stuck to the walls to prove it...

    I like the idea though..Maybe I can rig up a fire brick cage I can remove just before spinning the machine?

  4. #4
    Join Date
    Feb 2013
    Location
    Laidley, SE Qld
    Posts
    1,039

    Default

    If you've not been there, alloyavenue.com is a great source of info for all things DIY metal casting, the melting of brass is a well covered subject.

  5. #5
    Join Date
    Feb 2009
    Location
    Adelaide - outer south
    Age
    67
    Posts
    18

    Default

    Why can't you melt the metal in another furnace/crucible and then pour it into the crucible on the machine?

    Can you post a pic of the machine? It may help to illustrate the limitations / possibilities.
    Cheers, Bob the labrat

    Measure once and.... the phone rings!

Similar Threads

  1. Anyone have any experience casting brass?
    By Jim Ferrous in forum METALWORK GENERAL
    Replies: 7
    Last Post: 27th Sep 2013, 02:32 PM
  2. VICTORIA Brass Flat Bar Assorted Sizes & 1/4" SWB Threaded Rod & 260 Carbide Brass Sheet
    By thumbsucker in forum METALWORK - Machinery, Equipment, MARKET
    Replies: 7
    Last Post: 18th Mar 2013, 03:36 PM
  3. Casting about for cast iron casting ideas
    By Graziano in forum THE FOUNDRY
    Replies: 49
    Last Post: 1st Apr 2012, 12:05 PM
  4. Casting a brass nut.
    By Skew ChiDAMN!! in forum METALWORK GENERAL
    Replies: 6
    Last Post: 21st Nov 2011, 01:04 PM
  5. Replies: 12
    Last Post: 6th Nov 2011, 10:13 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •