Thanks: 0
Likes: 0
Needs Pictures: 0
Picture(s) thanks: 0
Results 16 to 16 of 16
-
30th May 2013, 11:25 PM #16
Nothing much to add, my experience is limited to lead and some forge work. A clagged vacuum makes a very good air source, hard to beat. i think the vacuum idea will work quite well and if it doesn't you probably will just need to fiddle with the air.