    Hi

    As I'm having a bit of an OCD moment, I was wondering if there is a convention for where the weight of a hammer head is stamped. I have a few sledge hammers and ball pein hammers to re-handle. Most of these have a weight stamped on them in ounces or pounds on a side where the hole for the handle is rather than on the cheek. I think that a lot of new sledges have the handle inserted from the marked side. Is this usual? Is there a reason for why it's done in a particular way? I know that in most cases for a "symmetrical" style hammer head it makes no difference, just interested, that's all.

    Simon

  2. #2
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    915

    Default

    Does not matter where the markings are although it does matter which way you insert the handle as the socket for the handle is tapered

  3. #3
    Join Date
    Feb 2009
    Location
    Tasmania
    Posts
    29

    Default

    Thanks China,

    I am aware of the taper in hammer heads. Are you suggesting that some hammer heads are tapered from one side only? I can't remember ever seeing one, not to say that they don't exist.

    As far as the weight marking goes, I can see where its position might be helpful when your put your hammers in a rack. Probably more for a "stocktake" purpose more that anything. I generally grab a hammer that's about the right size for what I want to do rather than worry about how much it weighs. Currently my hammer collection is spread about the workshop sitting on various horizontal surfaces and are mostly lost or misplaced when I want a particular one. I have at least 6 claw hammers, but don't ask me where they all are. I need a hammer rack of some sort, so it makes sense, perhaps to handle the hammer so that the weight shows when it's at home in the rack. My thinking for this is on the wedge side if you store hammers head upwards.... but most of my sledges are stored standing head down on the floor.

    Simon

  4. #4
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    915

    Default

    Yes some hammers are tapered in one direction only

  5. #5
    Join Date
    Oct 2001
    Location
    ACT
    Posts
    539

    Default

    different makers had a different place where they would put the weight markings. Hytest sledges generally had it on the side the handle was inserted from. Older cyclone ball peins were on what I call the left hand (side) face, then some later ones are marked in grams on the top large groove/fuller. many other hammer makers also put it on the left hand (side) face.

Similar Threads

  1. What weight hammer?
    By Michael G in forum METALWORK GENERAL
    Replies: 14
    Last Post: 9th Oct 2019, 07:24 AM
  2. Hammer head
    By eskimo in forum METALWORK GENERAL
    Replies: 6
    Last Post: 1st Apr 2018, 09:15 PM
  3. Can anyone identify these markings?
    By DSEL74 in forum METALWORK GENERAL
    Replies: 25
    Last Post: 3rd Feb 2014, 05:56 PM
  4. Bolt Markings
    By dazzler in forum METALWORK GENERAL
    Replies: 10
    Last Post: 29th Sep 2011, 04:52 PM
  5. Weight of HM-45 Head
    By Sterob in forum METALWORK GENERAL
    Replies: 6
    Last Post: 25th Dec 2007, 01:08 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •