    Default Gas Forge Build

    Made a start on my gas forges today. Both are having front opening doors and a fixed size mouth.

    Working out the hinges.








    …..Live a Quiet Life & Work with your Hands

  2. #2
    Join Date
    Dec 2007
    Location
    Melbourne
    Posts
    1,628

    Default





    Hinges started, sitting on the front mouth with the rear mouth inside.
    …..Live a Quiet Life & Work with your Hands

  3. #3
    Join Date
    Dec 2007
    Location
    Melbourne
    Posts
    1,628

    Default

    Hinges are done hinges just need to notch out the front to follow the curve.

    Hinge is made to match the width of the forge mouth.





    Next I need to make the feet and fit them so I can set the baseline foe horizontal to which the mouth can be cut parallel and the hinge pin at 90deg. Only problem is I have to wait for a non fireban day to light the coke forge to bend the feet.Gas Forge Build
    …..Live a Quiet Life & Work with your Hands

  4. #4
    Join Date
    Dec 2007
    Location
    Melbourne
    Posts
    1,628

    Default

    Got the feet bent up today along with forging a rebar filleting knife 🔪

    …..Live a Quiet Life & Work with your Hands

  5. #5
    Join Date
    Jan 2004
    Location
    Mackay North Qld
    Posts
    6,446

    Default

    It looks like a smooth move with the hinges if I am seeing it correctly.

    Its always easier to cut partially cut through the cylinder wall under the hinge area, tack hinges on,then complete the cut.

    No problems with misaligned or sagging doors

    It prevents all manner of grief from trying to match the door back to its original position and alignment.

    Will the D shaped door be hinged also?

    Grahame

  6. #6
    BobL is online now Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,189

    Default

    Quote Originally Posted by Grahame Collins View Post
    It looks like a smooth move with the hinges if I am seeing it correctly.

    Its always easier to cut partially cut through the cylinder wall under the hinge area, tack hinges on,then complete the cut.

    No problems with misaligned or sagging doors
    I just upgraded the camping fireplace/oven and did exactly that.
    This unit is made from a pair of SS clothes dryer drums.
    Every year I upgrade or mod it so there is something to talk about around the fire side.
    The complaint from the punters last year was that a single doorway did not allow for happy fireside ambience to be shared by everyone sitting around the campfire so the latest model has 3 doors that each cover about 50º each spread evenly around the shell of the fireplace.
    The top (oven) compartment is unchanged from last year.
    Will post come pics when I get the camera out.

  7. #7
    Join Date
    Dec 2007
    Location
    Melbourne
    Posts
    1,628

    Default

    plan was to fit the hinges before cutting the last few tabs that held the door on but that left me with a guess as to the location of the mouth. So I cut the door off today. New plan is to line it and fit the floor measure the height. Tack the door back in place cut the mouth and fit the hinges.


    …..Live a Quiet Life & Work with your Hands

  8. #8
    BobL is online now Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,189

    Default

    I welded a 25 mm wide ring as an internal rim on the open ends of the cylinder. Placed the ends (both my ends are on hinges) back on so it sat over the rim and welded the hinges in place. A complete rim is not really necessary - just 3 short tabs would do.

  9. #9
    Join Date
    Dec 2007
    Location
    Melbourne
    Posts
    1,628

    Default

    Rear opening in, went over it several times until I was running nice beads. Then ground the whole thing smoothing. No one will know I actually had nice welding for once

    …..Live a Quiet Life & Work with your Hands

  10. #10
    Join Date
    Dec 2007
    Location
    Melbourne
    Posts
    1,628

    Default

    Made some progress. Bought some cheap Chinese rods. Never waste your money on those. Had some experienced welders try them and couldn't get them to work either. As a beginner it really messed with my progress learning as I thought it was me.





    …..Live a Quiet Life & Work with your Hands

  11. #11
    Join Date
    Jan 2004
    Location
    Mackay North Qld
    Posts
    6,446

    Default

    DSEL74
    A question,if you will,on the length of that burner tube. Is there a particular reason why it is so long? is there a diameter to length ratio that affects the performance of the burner.

    Or is it that, you got the dimensions from a plan and are simply using those dimensions?

    I would like to find the reason as I am building one and want to keep the burner tube length short as possible to make it easier to wheel the furnace on its trolley into my storage space when I am not using it.

    A long burner tube sticking out may will catch on other things.

    Your furnace is coming very nicely.About the RHS inserted inside.

    Is it to provide a robust working surface or is there another reason?
    I am curious as to whether it will soak up a lot of energy getting it up to furnace running temp?

    Thanks
    Grahame

  12. #12
    Join Date
    Dec 2007
    Location
    Melbourne
    Posts
    1,628

    Default Gas Forge Build

    Sorry I can't really help on your burner question as I bought it like that from gameco. I was going to make one but after reading many posts on how much trouble people had tuning them and getting them to work properly I decided to buy what I had seen work on the same basic size and design forge. Corin works in the gas industry and makes forges and knives so I assume he knew what he was doing in terms of the gas flow etc.

    The tube unscrews from the Bing in the top of the forge so a little hassle but you could remove it for storage.

    The RHS in the front and rear is to create a strong opening where the tongs and steel will knock about rather than damaging the wool and have fibres blow off which can be harmful to breath.

    The reason it is angled is my hair brained idea of supporting long objects on one side and access with tongs on the other. I intend to cut away most of the protruding top and leave just the shelf and part of the side as a brace.
    When running the "dragons breath" does come out the door a good 100-200mm so the shel also shields your bench.

    I still have to coat mine with a wash of satanite, trim the RHS, and add a ring around the door, and a latch for the door.
    …..Live a Quiet Life & Work with your Hands

  13. #13
    Ueee's Avatar
    Ueee is offline Blacksmith, Cabinetmaker, Machinist, Messmaker
    Join Date
    Dec 2011
    Location
    Canberra
    Age
    40
    Posts
    4,515

    Default

    Whilst these burners screw in i would make it so they slip in to a bit of pipe welded into the body. This way you can just slip the burner out after use, it saves the important end from getting too hot after the forge is turned off. It will stay cold during use due to the cooling effect of the gas jet.

    Dale your RHS in your door should have the inner end covered with wool, any exposed steel will disappear at an alarming rate.
    1915 17"x50" LeBlond heavy duty Lathe, 24" Queen city shaper, 1970's G Vernier FV.3.TO Universal Mill, 1958 Blohm HFS 6 surface grinder, 1942 Rivett 715 Lathe, 14"x40" Antrac Lathe, Startrite H225 Bandsaw, 1949 Hercus Camelback Drill press, 1947 Holbrook C10 Lathe.

  14. #14
    Join Date
    Dec 2007
    Location
    Melbourne
    Posts
    1,628

    Default

    Bugger, can I get away with coating it with satanite?
    …..Live a Quiet Life & Work with your Hands

  15. #15
    Join Date
    Dec 2007
    Location
    Melbourne
    Posts
    1,628

    Default

    Gassed up the gas forge today, even made lunch.


    …..Live a Quiet Life & Work with your Hands

Page 1 of 2 12 LastLast

Similar Threads

  1. help me build a basic flat build bed trailer for my kayaks
    By gros21 in forum TRAILERS & OTHER FABRICATED STUFF
    Replies: 7
    Last Post: 13th Oct 2011, 08:47 AM
  2. Charcoal Forge
    By RayG in forum METALWORK GENERAL
    Replies: 29
    Last Post: 25th Jul 2009, 10:10 AM
  3. Trailer - to build or not to build
    By motegi in forum TRAILERS & OTHER FABRICATED STUFF
    Replies: 17
    Last Post: 6th May 2009, 03:07 PM
  4. New old forge
    By Andy Mac in forum THE SMITHY
    Replies: 8
    Last Post: 17th Apr 2009, 12:08 AM
  5. Forge
    By JB in forum THE SMITHY
    Replies: 28
    Last Post: 21st May 2005, 07:55 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •