    My Nephew came over today and we knocked up a charcoal forge for him to play about with.
    He did the cutting/drilling/sanding and I did the small bit of turning and the welding and we managed to finish by 5pm.

    I let the nephew set the height and it was his idea to include the removable galv ash guard around the top so I let him go with it.

    The blower is the one I constructed last week and detailed in a previous thread.
    View1.jpg

    The whole thing is built around a standard plough disc with a 150 mm diam octagon cut into and recessed by 50 mm.
    Air is fed from underneath via a 50 mm diam pipe
    outlet.jpg
    I recommended the 3 hole removable air outlet, and that 9 hole jobby is my nephew's design.

    Nick.jpg
    Nephew is pretty tall but I still think the forge is too tall for him, if it is he can cut off some of the leg length.

    Underneath.jpg
    Pretty standard underneath with a flippable ash trap door and air attachment

    Just another view
    View2.jpg

    If the tripod stand looks crooked, it is.
    Nephew was in a hurry to get it home so I just winged the angles on the stand.
    Being tripodular it is very stable.

    The rest is up to him.

  2. #2
    Join Date
    Nov 2006
    Location
    kansas mostly
    Posts
    33

    Default

    A question: Did you make sure the galvanized parts won't get hot enough to burn the zinc off? The fumes from overheated galvanized parts can cause respiratory problems (known as "metal fume fever"), limited exposure in someone healthy generally isn't life threatening but repeated exposure can cause long term problems.

    ron

  3. #3
    BobL is offline Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,189

    Default

    Quote Originally Posted by son_of_bluegras View Post
    A question: Did you make sure the galvanized parts won't get hot enough to burn the zinc off? The fumes from overheated galvanized parts can cause respiratory problems (known as "metal fume fever"), limited exposure in someone healthy generally isn't life threatening but repeated exposure can cause long term problems.

    ron
    Thanks for the concern. I'm aware of this as I have had a dose of this on a couple of occasions a few years back which is why I installed a vented welding booth in my shed.

    The galvanised ash shield won't get hot enough to form ZnO - you can see how far away it is from the fire in the pics below
    The shield will quickly become a PITA and I'm sure he will end up taking it off.

    The Galv pipe underneath the plough had the galvanising sanded off the hot end before welding the pipe to the recess.

    It would be better if there is no galv pipe used but the only 50 mm diam pipe I had was galvanised.
    The galv parts will probably still form a small amount of ZnO over time as the odd hot spark or coal falls onto them but as the forging will be done outside it should be OK.

    Said nephew was so eager to get started he went off an bought some charcoal and fired the forge up last night and his dad (BIL) sent me these photos.
    Heavens knows what the neighbours thought of all of all the clanging and hammering

    IMG_1127.jpg IMG_1126.jpg IMG_1125.jpg

  4. #4
    Join Date
    Dec 2009
    Location
    Sydney
    Posts
    327

    Default

    Neat!
    Shows how easy it is.
    A.
    'Waratah' spring hammer by Hands & Scott c.1911- 20, 'Duffy, Todd & Williams' spring hammer c.1920, Premo lathe- 1953, Premo filing machine.

  5. #5
    Join Date
    Jul 2013
    Location
    Perth
    Posts
    77

    Default The exuberance

    Ahh, "The Exuberance of Youth" Bob, if only we could bottle it and sell it to us old pharts eh!

    Good on you for "investing the time" into your nephew... who knows where it will lead, once he finds out about girls - he will likely forget about the metal or wood working skills for a decade or so (till the novelty wears off) BUT - once he has kids of his own and gets banished to the shed (like the rest of us), he will at least have some skills to fall back on. For this he will always thank his Uncle Bob!. Thats something $ can't buy!
    Definitely a effort.

    Cheers

  6. #6
    BobL is offline Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,189

    Default

    Quote Originally Posted by AndrewOC View Post
    Neat. Shows how easy it is.
    A.
    Yep - not that hard at all.

    Nephew Nick is a trainee stablehand/strapper and has seen farriers do their thing which got him thinking about doing some forging. His interests tend like a lot of young folks to jump around a bit so it wouldn't surprise me if he mucked about with forge for a few weeks and then moved onto something else. Despite this, the build experience albeit brief and too rushed for my liking was I think worthwhile.

    Of course he has now rung me up and wants tools, an anvil, etc , etc.

  7. #7
    Join Date
    Jul 2013
    Location
    Perth
    Posts
    77

    Default

    Of course he has now rung me up and wants tools, an anvil, etc , etc.
    Long as he works with you to make them - why not?.
    Making something with them - has far more value in todays easy come easy go world, than giving them something!
    If he invests time and effort into making something, he's more likely to look after it and keep it!.

  8. #8
    BobL is offline Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,189

    Default

    Quote Originally Posted by Timless Timber View Post
    Long as he works with you to make them - why not?.
    Making something with them - has far more value in todays easy come easy go world, than giving them something!
    If he invests time and effort into making something, he's more likely to look after it and keep it!.
    That's true although he's fairly scatter brain but I sense some improvement all round as he matures.

  9. #9
    Join Date
    Jul 2003
    Location
    Sydney
    Posts
    493

    Default

    Good minimalist approach to the forge build.
    A later improvement could be to add a square table around it, that is... a flat sheet with a round hole to fit the forge in, get rid of the ring around it and it can be held up buy some diagonals up from the legs. The table can have an edge of no more than 25mm in flat bar or even the same sheet bent up.
    The high rings around forges, just like those built with car rims, make heating the center of anything longer than the diameter of said ring a bummer.

    May I suggest a further gift for your nephew ?
    Buy him this book:
    The Backyard Blacksmith: Lorelei Sims: 9780785825678: Amazon.com: Books
    You can't go wrong with $8,90
    I got the book and read it cover to cover. When rather basic, it talks about most aspects of blacksmithing from the perspective of a professional with decades of experience, and being a woman, without the marble tower approach found in some of the gurus. Lorelei Sims - Artist/Blacksmith - BLACKSMITHCHIC.COM - Take a Tour of Five Points Blacksmith Shop
    Civilized man is the only animal clever enough to manufacture its own food,
    and the only animal stupid enough to eat it.
    Barry Groves

  10. #10
    BobL is offline Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,189

    Default

    Quote Originally Posted by Marc View Post
    Good minimalist approach to the forge build.
    A later improvement could be to add a square table around it, that is... a flat sheet with a round hole to fit the forge in, get rid of the ring around it and it can be held up buy some diagonals up from the legs. The table can have an edge of no more than 25mm in flat bar or even the same sheet bent up.
    The high rings around forges, just like those built with car rims, make heating the center of anything longer than the diameter of said ring a bummer.
    That sounds like pretty much like what I said to my nephew.

    The galv ring was his attempt to reduce ash scatter thereby keeping his parents off his back. They only have a small back yard and he's using the forge on a brick patio in between a pool and their shed. He says the ring helps. I suggested he reduced the height of the ring down to half an inch at two places on the ring opposite each other so that he can use these as a "pass thru" to heat longer things.

    May I suggest a further gift for your nephew ?
    Buy him this book:
    The Backyard Blacksmith: Lorelei Sims: 9780785825678: Amazon.com: Books
    You can't go wrong with $8,90
    I got the book and read it cover to cover. When rather basic, it talks about most aspects of blacksmithing from the perspective of a professional with decades of experience, and being a woman, without the marble tower approach found in some of the gurus. Lorelei Sims - Artist/Blacksmith - BLACKSMITHCHIC.COM - Take a Tour of Five Points Blacksmith Shop
    Sounds good - I'll look into it.

    Meanwhile he has had a go at forging some (medieval style) arrow tips for his long bow. This is no easy task as the metal section that wraps around the shaft has to be forged quite thin so he burnt a couple before succeeding in making one. I'm very pleased with his persistence although I worry about their neighbours.

  11. #11
    Join Date
    Jul 2003
    Location
    Sydney
    Posts
    493

    Default

    Quote Originally Posted by BobL View Post
    That sounds like pretty much like what I said to my nephew.

    The galv ring was his attempt to reduce ash scatter thereby keeping his parents off his back. They only have a small back yard and he's using the forge on a brick patio in between a pool and their shed. He says the ring helps. I suggested he reduced the height of the ring down to half an inch at two places on the ring opposite each other so that he can use these as a "pass thru" to heat longer things.


    Sounds good - I'll look into it.

    Meanwhile he has had a go at forging some (medieval style) arrow tips for his long bow. This is no easy task as the metal section that wraps around the shaft has to be forged quite thin so he burnt a couple before succeeding in making one. I'm very pleased with his persistence although I worry about their neighbors.
    Metalwork is a noisy business and blacksmith has the added noise from the anvil.
    When I don't know any way to quieten down an angle grinder, the anvil noise can be reduced a lot.
    If the anvil stump is replaced by a box filled with sand and a floating platform on top to sit the anvil on, the noise will reduce substantially to a dull knock.
    The ring can be suppressed with a large magnet under the horn or even a strip of tube rubber attached under the horn and stretched over it...providing you are not using it.
    I bet that quite angle grinders would have a big market if ever produced. I bet all it needs is a better gearbox.
    Civilized man is the only animal clever enough to manufacture its own food,
    and the only animal stupid enough to eat it.
    Barry Groves

  12. #12
    BobL is offline Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,189

    Default

    Quote Originally Posted by Marc View Post
    Metalwork is a noisy business and blacksmith has the added noise from the anvil.
    When I don't know any way to quieten down an angle grinder, the anvil noise can be reduced a lot.
    If the anvil stump is replaced by a box filled with sand and a floating platform on top to sit the anvil on, the noise will reduce substantially to a dull knock.
    The ring can be suppressed with a large magnet under the horn or even a strip of tube rubber attached under the horn and stretched over it...providing you are not using it.
    Thanks Marc, yeah I am aware of these strategies for anvil noise reduction. Also there is draping a heavy chain around the anvil, but his problem is he doesn't really have an anvil but a 16 mm thick, 150 x 150 mm U section about 300 mm long which rings like a giant tuning fork. I have suggested he clamp the two sides of the U together using some pieces of 4 x2 and a couple of 1/2" bolts - I haven't heard back from him about how that's going.

    I bet that quite angle grinders would have a big market if ever produced. I bet all it needs is a better gearbox.
    I agree - angle grinder noise is the pits.
    My solution to quiet metal cutting is where I can to use a small metal cutting bandsaw.
    Also I have an old 8" table saw that I put 125 mm thin kerf wheels into and it is much quieter than an angle grinder - not as portable but of course a lot safer and I can use it with water cooling if I need it. I still use angle grinders though but not as much as I used to.

  13. #13
    Join Date
    Jul 2003
    Location
    Sydney
    Posts
    493

    Default

    Quote Originally Posted by BobL View Post
    Thanks Marc, yeah I am aware of these strategies for anvil noise reduction. Also there is draping a heavy chain around the anvil, but his problem is he doesn't really have an anvil but a 16 mm thick, 150 x 150 mm U section about 300 mm long which rings like a giant tuning fork. I have suggested he clamp the two sides of the U together using some pieces of 4 x2 and a couple of 1/2" bolts - I haven't heard back from him about how that's going.


    I agree - angle grinder noise is the pits.
    My solution to quiet metal cutting is where I can to use a small metal cutting bandsaw.
    Also I have an old 8" table saw that I put 125 mm thin kerf wheels into and it is much quieter than an angle grinder - not as portable but of course a lot safer and I can use it with water cooling if I need it. I still use angle grinders though but not as much as I used to.
    Yes, he could also weld a flat bar across the U to stop the vibration.
    I never used a bandsaw but have a cold saw that makes life easier.
    Civilized man is the only animal clever enough to manufacture its own food,
    and the only animal stupid enough to eat it.
    Barry Groves

Similar Threads

  1. These bricks ok for a little forge?
    By RedShirtGuy in forum METALWORK GENERAL
    Replies: 8
    Last Post: 24th Feb 2011, 12:45 AM
  2. Gas Bottle Forge
    By Dingo Dog in forum METALWORK GENERAL
    Replies: 6
    Last Post: 26th Aug 2009, 04:39 PM
  3. Charcoal Forge
    By RayG in forum METALWORK GENERAL
    Replies: 29
    Last Post: 25th Jul 2009, 10:10 AM
  4. New old forge
    By Andy Mac in forum THE SMITHY
    Replies: 8
    Last Post: 17th Apr 2009, 12:08 AM
  5. Forge
    By JB in forum THE SMITHY
    Replies: 28
    Last Post: 21st May 2005, 07:55 PM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •