Small GAF block casting
As I said I would a while back (https://metalworkforums.com/f265/t20...cked-time-sort), I now have a price on the small GAF block castings that featured in two of my videos
DSCN8685 - Copy.JPG
The foundry has quoted $120 each for these, and postage/ freight will be necessary too if you can't pick up (roughly 3.5kg each). Offer is open until 1st July (soon after that they will be doing another cast iron run). Anyone interested will need to PM me. I will have to have money up front though. No offence but I can't afford to carry the cost of these if someone does not come through.
Michael
-
23rd Jun 2022, 10:29 PM #2
Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 55
- Posts
- 2,163
Any chance of a link to the video Michael?
I can't seem to find it.
Steve
-
23rd Jun 2022, 11:49 PM #3
China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,534
-
24th Jun 2022, 07:31 AM #4
Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 57
- Posts
- 6,154
Thanks Bob
and also https://www.youtube.com/watch?v=Swx8CMuStNU
Michael
-
24th Jun 2022, 02:50 PM #5
Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 70
- Posts
- 5,146
GAF transport
If anyone in the Melbourne area is wanting a set, and worried about the postage weight, I can take them over and deliver sometime after Michael gets them from the foundry.
I've already ordered my 2 sets.
HTH
KrynTo grow old is mandatory, growing up is optional.
-
24th Jun 2022, 08:37 PM #6
Intermediate Member
- Join Date
- Jun 2011
- Location
- Melbourne, Australia
- Posts
- 32
SA Small GAF block casting
Michael, I'll put my hand up for 2, please. For me it's a no brainer to support Australian made in favour of the import alternatives.
Salv
Similar Threads
-
Casting small amount its of brass
By BobL in forum THE FOUNDRYReplies: 7Last Post: 23rd Oct 2020, 10:53 AM -
Casting Tools Part 5 - Casting a part
By RayG in forum THE FOUNDRYReplies: 10Last Post: 30th Jul 2018, 12:46 PM -
Casting about for cast iron casting ideas
By Graziano in forum THE FOUNDRYReplies: 49Last Post: 1st Apr 2012, 12:05 PM -
Casting Tools Part 4 - Sand Casting Tools
By RayG in forum THE FOUNDRYReplies: 8Last Post: 9th Dec 2011, 12:03 PM -
Casting small engine parts
By wgipps in forum METALWORK GENERALReplies: 31Last Post: 1st Dec 2011, 02:26 PM