Greg. While they are cast iron, almost all of them are chilled cast iron and near impossible to machine.... just saying....
Cheers, Joe
retired - less energy, more time to contemplate projects and more shed time....
-
27th Feb 2021, 09:20 AM #4
There’s about 3 or 4 left now, I think.
Cheers Matt.
-
27th Feb 2021, 09:33 AM #5Golden Member
- Join Date
- Mar 2009
- Location
- Melbourne
- Age
- 54
- Posts
- 825
G’day Joe,
The bit about them mostly being chill cast is said a lot but I use them all the time and have only had problems now and then. They’re my go to source for plugs and patches when doing CI repairs and I’ve machined plenty of parts from them including piston rings
221679F2-DD4F-49D6-964F-B0FDD3FF747B.jpg
3F8F25C9-4239-4721-A739-295BEFCD8898.jpg
Sure they’re not always Flocast quality but I like the price a lot better.
Matt, if you can hang on to the the last 3 or 4 I’ll grab them from you on Monday if that’s ok?
Cheers,
Greg.
-
27th Feb 2021, 10:26 AM #6
Window weights all gone.
Cheers Matt.
-
28th Feb 2021, 12:05 AM #7
That is lucky - or I've been unlucky. I was talking from my own experience - which, as you say, is reflected in other posts. None of my stack could even be cut with a bandsaw.... so I stopped trying to use them. I contemplated putting them in our wood heater one winter and try and heat treat them for few days....
Cheers, Joe
retired - less energy, more time to contemplate projects and more shed time....
-
28th Feb 2021, 02:04 AM #8Most Valued Member
- Join Date
- Oct 2010
- Location
- melbourne, laverton
- Posts
- 1,910
-
28th Feb 2021, 10:56 AM #9
Glad these are steel cast. My experience has alwa6s been lead weights.
Similar Threads
-
Moving machines, weights
By j3dprints in forum METALWORK GENERALReplies: 12Last Post: 14th Mar 2019, 07:37 PM -
Welder about to go out the window
By gazza2009au in forum WELDINGReplies: 96Last Post: 26th Aug 2018, 02:20 PM -
Manufacturing spoke weights. How were these made?
By gjws in forum METALWORK GENERALReplies: 18Last Post: 15th Jan 2018, 04:43 AM -
rusty gym weights - any advice?
By Mindabout in forum METALWORK GENERALReplies: 10Last Post: 30th Apr 2010, 10:54 PM -
No new window?
By MajorPanic in forum FORUMS INFO, HELP, DISCUSSION & FEEDBACKReplies: 12Last Post: 11th Aug 2005, 05:53 PM